Back to results
US 2019/0316219 A1Published application
Thick steel plate having excellent cryogenic impact toughness and manufacturing method therefor
AssigneePosco
InventorsMo-Chang Kang, Jong-In Choi
Life of this patent
Estimating the term…
Abstract
The purpose of one aspect of the present invention is to provide: a thick steel plate capable of removing a conventional normalizing treatment required for ensuring toughness low temperature and cryogenic environments, and having properties equal to or better than those of a conventional steel subjected to the normalizing treatment; and a method for manufacturing the method.
Claims8
A thick steel plate having excellent cryogenic impact toughness, comprising:
- by weight %, 0.02% to 0.10 of carbon (C), 0.6 to 1.7% of manganese (Mn), 0.5% or less (excluding 0%) of silicon (Si), 0.02% or less of phosphorus (P), 0.015% or less of sulfur (S), 0.005 to 0.05% of niobium (Nb), 0.005 to 0.07% of vanadium (V), and a remainder of iron (Fe) and other unavoidable impurities,
- wherein the thick steel plate has, by area fraction, a mixed structure of ferrite of 85 to 95% and pearlite of 5 to 15%, as a microstructure.
A method of manufacturing a thick steel plate having excellent cryogenic impact toughness, comprising:
- reheating a steel slab at a temperature of 1100° C. or higher, the steel slab including, by weight %, 0.02% to 0.10 of carbon (C), 0.6 to 1.7% of manganese (Mn), 0.5% or less (excluding 0%) of silicon (Si), 0.02% or less of phosphorus (P), 0.015% or less of sulfur (S), 0.005 to 0.05% of niobium (Nb), 0.005 to 0.07% of vanadium (V), and a remainder of iron (Fe) and other unavoidable impurities,
- finishing hot-rolling the reheated steel slab at a temperature of 850 to 910° C. to produce a hot-rolled steel plate;
- and
- air-cooling the hot-rolled steel plate to a room temperature after the finishing hot-rolling.
1 more element
Dependencies are inferred from the claim text.