Preparation method of shape memory polyurethane
AssigneeShenzhen University
InventorsShaojun Chen, Shuqin Fu
Life of this patent
Estimating the term…
Loading patent…
AssigneeShenzhen University
InventorsShaojun Chen, Shuqin Fu
Estimating the term…
The present disclosure provides a preparation method of a shape memory polyurethane, which comprising: reacting 1,3,5,7-tetrahydroxyadamantane, ϵ-caprolactone, a catalyst and a solvent for 20-50 hours under the conditions of inert gas and 70° C. to 130° C. to obtain adamantyl star poly(ϵ-caprolactone), wherein the mole ratio of the 1,3,5,7-tetrahydroxyadamantane to the ϵ-caprolactone is 1:(40-240); mixing the adamantyl star poly(ϵ-caprolactone) with long-chain diol and diisocyanate, adding the catalyst and the solvent, and reacting for 3-9 hours at 50-100° C. to obtain an isocyanate-terminated polyurethane prepolymer, wherein the mass ratio of the adamantyl star poly(ϵ-caprolactone) to the long-chain diol is 9:1-1:9; and adding a linking agent in the polyurethane prepolymer so that the linking agent reacts with isocyanate in the polyurethane prepolymer to obtain an adamantyl cross-linked shape memory polyurethane.
A method for preparing a shape memory polyurethane comprising:
Dependencies are inferred from the claim text.