Use of a semi-aromatic polyamide in a mixture of aliphatic polyamide comprising circular-section glass fibres to limit warping
AssigneeArkema France
InventorsBenoît BRULE, Antoine BREUIL, Hao WANG, Xiong YAO
Life of this patent
Estimating the term…
Loading patent…
AssigneeArkema France
InventorsBenoît BRULE, Antoine BREUIL, Hao WANG, Xiong YAO
Estimating the term…
The use of at least one MXDZ polyamide, obtained from the polycondensation of meta-xylylenediamine (MXD), with a C6 to C18 aliphatic (Z) dicarboxylic acid, in particular C6 to C12, in a mixture including at least one aliphatic polyamide A obtained from the polycondensation of a unit selected from: a C6 to C12 lactam, a C6 to C12amino acid, and an XY unit obtained from the polycondensation of a C4 to C18, aliphatic diamine (X), especially C4 to C12, and a C6 to C18 aliphatic dicarboxylic acid (Y), especially C6 to C12, circular-section glass fibres and optionally at least one impact modifier and/or at least one additive, said at least one MXDZ polyamide and said mixture constituting a composition, and the MXDZ/A weight ratio being from 0.11 to 0.83, in particular from 0.11 to 0.66, to limit the warping of said composition during processing, in particular by injection or compression moulding.
Use of at least one MXDZ polyamide, obtained from the polycondensation of meta-xylylenediamine (MXD), with a C6 to C18 aliphatic (Z) dicarboxylic acid, in a mixture comprising at least one aliphatic polyamide A obtained from the polycondensation of a unit selected from:
Dependencies are inferred from the claim text.