High Flow Automotive Exterior Compounds with Excellent Surface Appearance
AssigneeBorealis AG
InventorsThomas Lummerstorfer, Daniela Mileva, Georg Grestenberger
Life of this patent
Estimating the term…
Abstract
The present invention is directed to propylene composition applicable for high flow automotive exterior compounds with excellent surface appearance, said composition comprising a modified polypropylene composition and an inorganic filler.
Claims17
Composition (C) comprising a modified polypropylene composition (mPP) and an inorganic filler (F), wherein said modified polypropylene composition (mPP) is obtained by treatment of a polypropylene composition (PP) with a peroxide (PO), said polypropylene composition (PP) comprising
- (a) a heterophasic composition (HECO), comprising
- (a1) a (semi)crystalline polypropylene (PP1) and
- (a2) an elastomeric ethylene/propylene copolymer (EPR) dispersed in said (semi)crystalline polypropylene (PP1),
- (b) a plastomer (PL) being a copolymer of ethylene and at least one C4 to C20 α-olefin, and
- (c) optionally a high flow polypropylene (HPP), said high flow polypropylene (HPP) has preferably a higher melt flow rate MFR2 (230° C.), measured according to ISO 1133, than the (semi)crystalline polypropylene (PP1).
Composition (C) comprising a modified polypropylene composition (mPP) and an inorganic filler (F), wherein said modified polypropylene composition (mPP) is obtained from a polypropylene composition (PP) comprising
- (a) a heterophasic composition (HECO), comprising
- (a1) a (semi)crystalline polypropylene (PP1) and
- (a2) an elastomeric ethylene/propylene copolymer (EPR) dispersed in said (semi)crystalline polypropylene (PP1),
- (b) a plastomer (PL) being a copolymer of ethylene and at least one C4 to C20 α-olefin, and
- (c) optionally a high flow polypropylene (HPP), said high flow polypropylene (HPP) has preferably a higher melt flow rate MFR2 (230° C.), measured according to ISO 1133, than the (semi)crystalline polypropylene (PP1),
- wherein the modified polypropylene composition (mPP) has
- (i) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 above 32 g/10 min, and
- (ii) a ratio IV(XCS)/IV(XCI) of at least 2.10, wherein IV(XCS) is the intrinsic viscosity IV determined according to DIN ISO 1628/1 (in Decalin at 135° C.) of the xylene soluble fraction XCS and IV(XCI) is the intrinsic viscosity IV determined according to DIN ISO 1628/1 (in Decalin at 135° C.) of the xylene insoluble fraction XCI.
Composition (C) according to any one of the preceding claims, wherein said plastomer (PL) is a copolymer of ethylene and 1-butene or 1-octene.
Composition (C) according to any one of the preceding claims, wherein the modified polypropylene composition (mPP) has
- (i) an intrinsic viscosity IV determined according to DIN ISO 1628/1 (in Decalin at 135° C.) of the xylene soluble fraction XCS below 2.30 dl/g and
- (ii) an intrinsic viscosity IV determined according to DIN ISO 1628/1 (in Decalin at 135° C.) of the xylene insoluble fraction XCI below 1.05 dl/g.
Composition (C) according to any one of the preceding claims, wherein the weight ratio of the heterophasic composition (HECO) and the plastomer (PL) [(HECO)/(PL)] in the polypropylene composition (PP) is in the range of 0.1 to 10.0.
Composition (C) according to any one of the preceding claims, wherein the polypropylene composition (PP) comprises 3 to 15 wt.-%, based on the overall weight of the polypropylene composition (PP), of the high flow polypropylene (HPP) preferably having a higher melt flow rate MFR2 (230° C.), measured according to ISO 1133, than the (semi)crystalline polypropylene (PP1).
Composition (C) according to any one of the preceding claims, comprising
- (a) 45 to 95 wt.-% of the modified polypropylene composition (mPP) and
- (b) 5 to 30 wt.-% of the inorganic filler (F),
- based on the overall weight of the composition (C).
Composition (C) according to any one of the preceding claims, wherein the heterophasic composition (HECO) has
- (a) a comonomer content, based on the total weight of the heterophasic composition (HECO), in the range of 3 to 20 wt.-%,
- and/or
- (b) a xylene soluble fraction (XCS) in the range of 10 to 35 wt.-%,
- and/or
- (c) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 from 40 to 100 g/10 min
Composition (C) according to any one of the preceding claims, wherein the xylene soluble fraction (XCS) of the heterophasic composition (HECO) has
- (a) an intrinsic viscosity (IV) determined according to DIN ISO 1628/1 (in Decalin at 135° C.) in the range of 1.5 to 4.5 dl/g,
- (b) a comonomer content, based on the total weight of the xylene soluble fraction (XCS) of the heterophasic composition (HECO), in the range of 25 to 55 wt.-%.
Composition (C) according to any one of the preceding claims, wherein the plastomer (P) has
- (a) a melt flow rate MFR (190° C.) measured according to ISO 1133 from 0.05 to 5.0 g/10 min
- (b) a comonomer content, based on the total weight of the plastomer (PL), in the range of 5 to 25 mol-% and
- (c) a density equal or below 0.880 g/cm3.
Composition (C) according to any one of the preceding claims, wherein the inorganic filler (F) is talc.
Dependencies are inferred from the claim text.