US 2019/0241705 A1Published application
Polyamide acid, polyamide acid solution, polyimide, polyimide film, laminate, flexible device, and method of manufacturing polyimide film
AssigneeKaneka Corporation
InventorMari UNO
Life of this patent
Estimating the term…
Abstract
A polyamide acid of the present invention contains, as a diamine component, 2,2-bistrifluoromethylbenzidine and trans-1,4-cyclohexanediamine, and contains, as a tetracarboxylic acid dianhydride component, a pyromellitic acid anhydride and a 3,3,4,4-biphenyltetracarboxylic acid dianhydride. A ratio of the trans-1,4-cyclohexanediamine to a total amount of the diamine is preferably 0.5-40 mol %. A polyimide is obtained by dehydration ring closure of the polyamide acid.
Claims20
1:
- A polyamide acid that is a polyaddition reaction product of a diamine and a tetracarboxylic acid dianhydride, wherein
- the diamine comprises 2,2-bistrifluoromethylbenzidine and trans-1,4-cyclohexanediamine, and
- the tetracarboxylic acid dianhydride comprises a pyromellitic acid anhydride and a 3,3,4,4-biphenyltetracarboxylic acid dianhydride.
2:
- The polyamide acid according to claim 1, wherein a ratio of the trans-1,4-cyclohexanediamine to a total amount of the diamine is from 0.5 to 40 mol %.
3:
- The polyamide acid according to claim 1, wherein, in the tetracarboxylic acid dianhydride, a ratio of the pyromellitic acid anhydride to a total of 100 mol % of the pyromellitic acid anhydride and the 3,3,4,4-biphenyltetracarboxylic acid dianhydride is from 5 to 80 mol %.
4:
- A polyamide acid solution, comprising:
- the polyamide acid according to claim 1;
- and
- an organic solvent.
1 more element
5:
- The polyamide acid solution according to claim 4, further comprising:
- an imidazole.
6:
- The polyamide acid solution according to claim 5, wherein a content of the imidazole with respect to 1 mole of an amide group of the polyamide acid is 0.10 moles or less.
7:
- A polyimide that is a polycondensation reaction product of a diamine and a tetracarboxylic acid dianhydride, wherein
- the diamine comprises 2,2-bistrifluoromethylbenzidine and trans-1,4-cyclohexanediamine, and
- the tetracarboxylic acid dianhydride comprises a pyromellitic acid anhydride and a 3,3,4,4-biphenyltetracarboxylic acid dianhydride.
8:
- The polyimide according to claim 7, wherein a ratio of the trans-1,4-cyclohexanediamine to a total amount of the diamine is from 0.5 mol % to 40 mol %.
9:
- The polyimide according to claim 7, wherein, in the tetracarboxylic acid dianhydride, a ratio of the pyromellitic acid anhydride to a total of 100 mol % of the pyromellitic acid anhydride and the 3,3,4,4-biphenyltetracarboxylic acid dianhydride is from 5 to 80 mol %.
10:
- A polyimide film, comprising:
- the polyimide according to claim 7.
11:
- The polyimide film according to claim 10, wherein
- a light transmittance at a wavelength of 450 nm of the polyimide film is 75% or more,
- a haze of the polyimide film is 1.2% or less, and
- a coefficient of thermal expansion of the polyimide film during temperature rising and a coefficient of thermal expansion of the polyimide film during temperature lowering at 100-300° C. are 15 ppm/K or less.
1 more element
12:
- A laminate, comprising:
- a base material;
- and
- the polyimide film according to claim 10 provided on the base material.
1 more element
13:
- A flexible device, comprising:
- the polyimide film according to claim 10;
- and
- an electronic element provided on the polyimide film.
1 more element
14:
- A method for manufacturing a polyimide film, comprising:
- forming a laminate by applying the polyamide acid solution according to claim 4 onto a base material to provide a film-like polyamide acid on the base material;
- and
- heating the laminate to imidize the polyamide acid.
1 more element
15:
- A method for manufacturing a polyimide film, comprising:
- forming a polyimide film by the method according to claim 14;
- and
- separating the base material from the polyimide film.
1 more element
16:
- The method for manufacturing a polyimide film according to claim 15, wherein the separating of the base material from the polyimide film is performed by laser irradiation.
17:
- The polyamide acid according to claim 1, wherein a ratio of the trans-1,4-cyclohexanediamine to a total amount of the diamine is from 1.0 to 35 mol %.
18:
- The polyamide acid according to claim 1, wherein a ratio of the trans-1,4-cyclohexanediamine to a total amount of the diamine is from 5 to 25 mol %.
19:
- The polyamide acid according to claim 1, wherein, in the tetracarboxylic acid dianhydride, a ratio of the pyromellitic acid anhydride to a total of 100 mol % of the pyromellitic acid anhydride and the 3,3,4,4-biphenyltetracarboxylic acid dianhydride is from 10 to 70 mol %.
20:
- The polyamide acid according to claim 1, wherein, in the tetracarboxylic acid dianhydride, a ratio of the pyromellitic acid anhydride to a total of 100 mol % of the pyromellitic acid anhydride and the 3,3,4,4-biphenyltetracarboxylic acid dianhydride is from 20 to 60 mol %.