An iron-based steel comprising at least (in wt. %): carbon (C): 0.01%-0.10%; silicon (Si): 0.02%-0.7%; manganese (Mn): 0.3%-1.0%; chromium (Cr): 8.0%-10%; molybdenum (Mo): 0.1%-1.8%; cobalt (Co): 0.8%-2.0%; nickel (Ni): 0.008% -0.20%; boron (B): 0.004% -0.01%; nitrogen (N): 0.03% -0.06%; vanadium (V): 0.1% -0.3%, particularly 0.15% -0.022% of vanadium (V), more particularly 0.185% of vanadium (V); niobium (Nb): 0.01% -0.07%; optionally tungsten (W): 2.0% -2.8%, particularly 2.4% of tungsten; the remainder being iron (Fe); wherein said steel consists in particular of these elements.
An iron-based alloy comprising at least (in % by weight):
Dependencies are inferred from the claim text.