Method for producing fusible material for three-dimensional molding
AssigneeKao Corporation
InventorsTomoya TSUBOI, Jouji HIRAI, Takuma KIMURA, Tadanori YOSHIMURA, Akihiro ONOUE
Life of this patent
Estimating the term…
Loading patent…
AssigneeKao Corporation
InventorsTomoya TSUBOI, Jouji HIRAI, Takuma KIMURA, Tadanori YOSHIMURA, Akihiro ONOUE
Estimating the term…
The method for manufacturing a soluble material for three-dimensional modeling that is used as a material of a support material that supports a three-dimensional object when manufacturing the three-dimensional object with a 3D printer of a fused deposition modeling system, comprising a kneading step of kneading raw materials of the soluble material for three-dimensional modeling by a twin screw extruder having a screw configuration in which a ratio of a total length K of kneading discs to a total length L of an effective screw is 0.20<K/L<0.70 and in which a temperature Tmix of the raw materials of the soluble material for three-dimensional modeling in the kneading step and a glass transition temperature Tg of a base polymer contained in the raw materials of the soluble material for three-dimensional modeling satisfy a formula Tg+80(° C.)<Tmix<Tg+200(° C.).
A method for manufacturing a soluble material for three-dimensional modeling that is used as a material of a support material that supports a three-dimensional object when manufacturing the three-dimensional object with a 3D printer of a fused deposition modeling system, comprising a kneading step of kneading raw materials of the soluble material for three-dimensional modeling by a twin screw extruder having a screw configuration in which a ratio of a total length K of kneading discs to a total length L of an effective screw is 0.20<K/L<0.70 and in which a temperature Tmix of the raw materials of the soluble material for three-dimensional modeling in the kneading step and a glass transition temperature Tg of a base polymer contained in the raw materials of the soluble material for three-dimensional modeling satisfy a formula Tg+80(° C.)<Tmix<Tg+200(° C.).
Dependencies are inferred from the claim text.