Clay plaster and a method of its realization
AssigneeFormes SP. Z O.O
InventorAndrzej SROCZYNSKI
Life of this patent
Estimating the term…
Loading patent…
AssigneeFormes SP. Z O.O
InventorAndrzej SROCZYNSKI
Estimating the term…
The object of the invention is a clay plaster and a method of performing the clay plaster, wherein the clay plaster comprising clay and optionally aggregates in the form of sand, organic and/or mineral fillers, characterizes in that it comprises clay in an amount of more than 40% by weight, preferably more than 60% by weight, and more preferably more than 80% by weight, and most preferably 100% by weight of content based on the clay plaster dry matter, wherein the clay is in a powder form and granular form, whereby the amount of clay powder does not exceed 80% by weight of the granular clay and optionally comprises a mineral and/or organic filler in an amount of not more than 60% by weight, as well as possible modifying additives, additives increasing the adhesion to the substrate, additives delaying the time of granular clay soaking, retention additives and/or pigments, wherein the amount of additives is not more than 10% by weight based on the clay plaster dry matter and the method of performing the clay plaster according to the invention consists in rapid mixing of the dry ingredients of the clay plaster with an aqueous solvent immediately prior to its application to or during application onto the substrate. Thus mixed clay plaster, before the clay grains soaking in and humidity homogenisation, is immediately applied onto the substrate prepared as for other mineral plasters, resulting in a good adhesion to the substrate after drying. Preferably, the clay plaster is applied onto the substrate after having applied a bonding layer in the form of clay slurry onto a dry substrate first.
A clay plaster comprising:
(canceled)
(canceled)
(canceled)
The method according to claim 13, wherein the clay plaster is applied onto the substrate after having applied a bonding layer in the form of clay slurry onto a dry substrate first.
The method according to claim 13, wherein the levelling layer has a thickness of 3mm to 60 mm and is applied manually or mechanically onto the substrate with simultaneous surface levelling.
The method according to claim 13, wherein the aqueous solvent is in the form of a clay slurry with a liquid consistency, being a mixture of water and clay, and wherein the dry clay content is over 10% by volume in relation to the fillers.
A method of applying a clay plaster onto a substrate, said clay plaster having clay in an amount of more than 40% by weight of content based on clay plaster dry matter, wherein the clay is in a powder form having grain size of up to 1.5 mm and granular form having grain size larger than 1.5 mm up to grain size not exceeding the thickness of a layer of clay plaster which is to be applied to a substrate, whereby the amount of clay in powder form does not exceed 80% by weight of the clay in granular form, said clay plaster including no more than 60% by weight of aggregates in the form of a mineral and/or organic filler, and said clay plaster including no more than 10% by weight, based on the clay plaster dry matter, of modifying additives for increasing the adhesion to the substrate, for delaying the time of granular clay soaking, retention additives and/or pigments, said method comprising the steps of:
Dependencies are inferred from the claim text.