Anode, battery, and method of manufacturing same
AssigneeSony Corporation
InventorsKenichi Kawase, Yukiko lijima
Life of this patent
Estimating the term…
Abstract
A battery capable of improving cycle characteristics is provided. An anode active material layer is formed by forming a precursor layer containing active material particles containing Si and Li as an element, and then heating the resultant. Thereby, the active material particles are bound to each other by sintering or fusing, and united three-dimensionally. Since Li is contained therein, the active material particles can be sufficiently sintered even if the heating temperature is low, 600 deg C.
Claims14
A method of manufacturing an anode including:
- providing a precursor layer containing anode active material particles containing silicon (Si) and lithium (Li) on an anode current collector;
- heating the precursor layer;
- and
- binding the anode active material particles to each other by sintering or fusing to form an anode active material layer.
A method of manufacturing a battery comprising a cathode, an anode, and an electrolyte, the method comprising:
- forming an anode by (a) providing a precursor layer containing anode active material particles containing silicon (Si) and lithium (Li) on an anode current collector, (b) heating the precursor layer, and (c) binding the anode active material particles to each other by sintering or fusing to form an anode active material layer;
- and
- assembling the cathode, the anode, and the electrolyte into the battery.
Dependencies are inferred from the claim text.