Back to results
US 2017/0321347 A1Published application
Isoelectronic surfactant induced sublattice disordering in optoelectronic devices
AssigneeThe Boeing Company
InventorsChristopher M. FETZER, James H. ERMER, Richard R. KING, Peter C. COLTER
Life of this patent
Estimating the term…
Abstract
A method of disordering a layer of an optoelectronic device including; growing a plurality of lower layers; introducing an isoelectronic surfactant; growing a layer; allowing the surfactant to desorb; and growing subsequent layers all performed at a low pressure of 25 torr.
Claims20
A method of making a III-V optoelectronic device, comprising:
- growing a lower structure;
- introducing an isoelectronic surfactant in a molar ratio of isoelectronic surfactant to group-III precursor that is between about 1×10−5 to 0.2;
- and
- growing a subsequent structure at a reduced pressure of 10 to 100 torr in the presence of the isoelectronic surfactant;
- wherein a band gap associated with the subsequent structure is increased by a disordering induced by the isoelectronic surfactant to substantially match a photogenerated current between the subsequent structure and one or more other layers;
- wherein the subsequent structure is characterized by an ordering parameter η that is at most about 0.3;
- and
- wherein any remaining CuPtB-type ordering of the subsequent structure produces at most 0.100 eV of band gap reduction from a disordered alloy maximum.
5 more elements
A method of making a III-V optoelectronic device, comprising:
- growing a lower structure;
- growing a first side and a second side of a tunnel junction;
- introducing an isoelectronic surfactant in a molar ratio of isoelectronic surfactant to group III precursor that is between about 1×10−5 to 0.2;
- increasing a band gap associated with a top structure by growing the top structure in the presence of the isoelectronic surfactant at a pressure of 10 to 100 torr;
- and
- growing a subsequent structure:
- wherein the band gap associated with the top structure is increased by a disordering induced by the isoelectronic surfactant to substantially match a photogenerated current between the top structure and one or more other layers;
- wherein the top structure is characterized by an ordering parameter 11 that is at most about 0.3;
- and
- wherein any remaining CuPtB-type ordering of the subsequent structure produces at most 0.100 eV of band gap reduction from a disordered alloy maximum.
7 more elements
A method of making a solar cell having a GainP top layer, comprising:
- growing a lower structure;
- introducing an isoelectronic surfactant selected from the group consisting of Sb, As, Bi, Tl, the isoelectronic surfactant being present in a molar ratio of isoelectronic surfactant to group III precursor that is at least 1×10−5;
- and
- growing a subsequent structure at a reduced pressure of 10 to 100 torr in the presence of the isoelectronic surfactant that comprises a top layer,
- wherein the top layer comprises GaInP:
- wherein a band gap associated with the top layer is increased by a disordering induced by the isoelectronic surfactant to substantially match a photogenerated current between the top layer and one or more other layers;
- wherein the top layer is characterized by an ordering parameter 11 that is at most about 0.3;
- and
- wherein any remaining CuPtB-type ordering of the subsequent structure produces at most 0.100 eV of band gap reduction from a disordered alloy maximum.
6 more elements