An amorphous soft magnetic alloy of the formula (Fe1-αTMα)100-w-x-y-zPwBxLySiz TipCqMnrCus, wherein TM is Co or Ni; L is Al, Cr, Zr, Mo or Nb; 0≦α≦0.3, 2≦w≦18 at %, 2≦x≦18 at %, 15≦w+x≦23 at %, 1<y≦5 at %, 0≦z≦4 at %; p, q, r, and s represents an addition ratio such that the total mass of Fe, TM, P, B, L and Si is 100, and 0≦p≦0.3, 0≦q≦0.5, 0≦r≦2, 0≦s≦1 and r+s>0; the composition fulfills one of the following conditions: L is Cr, Zr, Mo or Nb; or L is a combination of Al and Cr, Zr, Mo or Nb, wherein 0<Al≦5 at %, 1≦Cr≦4 at %, 0<Zr≦5 at %, 2≦Mo≦5 at %, and 2≦Nb≦5 at %; the alloy has a crystallization start temperature (Tx) which is 550° C. or less, a glass transition temperature (Tg) which is 520° C. or less, and a supercooled liquid region represented by ΔTx=Tx−Tg, which is 20° C. or more.
An amorphous soft magnetic alloy comprising a composition expressed by a formula of (Fe1-αTMα)100-w-x-y-zPwBxLySizTipCqMnrCus, wherein unavoidable impurities are contained, TM is at least one element selected from the group consisting of Co and Ni, L is at least one element selected from the group consisting of Al, Cr, Zr, Mo, and Nb, wherein 0≦α≦0.3, 2≦w≦18 at %, 2≦x≦18 at %, 15≦w+x≦23 at %, 1<y≦5 at %, 0≦z≦4 at %, and p, q, r, and s each represents an addition ratio such that the total mass of Fe, TM, P, B, L and Si is 100, and are defined as 0≦p≦0.3, 0≦q≦0.5, 0≦r≦2, 0≦s≦1 and r+s>0, and said composition fulfills one of the following conditions (A) and (B):