Polyimide fibre and method for producing polyimide fibre
AssigneeI.S.T. Corporation
InventorsRyuta NAKAGAKI, Katsuki MORISHIMA, Koji MORIUCHI
Life of this patent
Estimating the term…
Loading patent…
AssigneeI.S.T. Corporation
InventorsRyuta NAKAGAKI, Katsuki MORISHIMA, Koji MORIUCHI
Estimating the term…
The method for producing a polyimide fiber includes a coagulation step of forming a polyimide precursor fiber by extruding a polyimide precursor solution containing a polyimide precursor and a compound having an acid dissociation constant (pKa) of a conjugate acid in water at 25° C. of 6.0 to 10 inclusive and an octanol-water partition coefficient (Log P) at 25° C. of −0.75 to 0.75 inclusive into a poor solvent or nonsolvent for the polyimide precursor; and a heat drawing step of forming the polyimide fiber by drawing the polyimide precursor fiber while heating same. The polyimide fiber of the present disclosure has a physical property such that the coefficient of thermal expansion thereof is in the range of −15 ppm/K to 0 ppm/K inclusive.
A polyimide fiber having a coefficient of thermal expansion in the range of −15 ppm/K to 0 ppm/K inclusive.
A method for producing a polyimide fiber comprising:
A method of using, in production of a polyimide fiber using a polyimide precursor solution as a starting material, a compound having an acid dissociation constant (pKa) of a conjugate acid in water at 25° C. in the range of 6.0 to 10 inclusive and an octanol-water partition coefficient (Log P) at 25° C. in the range of −0.75 to 0.75 inclusive as a coagulation alleviating agent of a polyimide precursor in the polyimide precursor solution.
Dependencies are inferred from the claim text.