Copper alloy sheet material and method of manufacturing the same
AssigneeJX Nippon Mining & Metals Corporation
InventorKEI SAEGUSA
Life of this patent
Estimating the term…
Loading patent…
AssigneeJX Nippon Mining & Metals Corporation
InventorKEI SAEGUSA
Estimating the term…
A copper alloy sheet material includes 0.5 to 2.5 mass % of Ni, 0.5 to 2.5 mass % of Co, 0.30 to 1.2 mass % of Si and 0.0 to 0.5 mass % of Cr and the balance Cu and unavoidable impurities, wherein an X-ray diffraction intensity ratio is 1.0≦I{200}/I0{200}≦5.0 when I{200} is a result of the X-ray diffraction intensity of {200} crystal plane of sheet surface and I0{200} is a result of the X-ray diffraction intensity of {200} crystal plane of a standard powder of pure copper, and wherein 0.2% yield strength in a rolling parallel direction (RD) is 800 MPa or more and 950 MPa or less, an electrical conductivity of 43.5% IACS or more and 53.0% IACS or less, 180 degree bending workability in a rolling parallel direction (GW) and a rolling perpendicular direction (BW) is R/t=0, and a difference between the rolling parallel direction (RD) and a rolling perpendicular direction (TD) of the 0.2% yield strength is 40 MPa or less.
A copper alloy sheet material comprising 0.5 to 2.5 mass % of Ni, 0.5 to 2.5 mass % of Co, 0.30 to 1.2 mass % of Si and 0.0 to 0.5 mass % of Cr, and the balance Cu and unavoidable impurities, wherein an X-ray diffraction intensity ratio is 1.0≦I{200}/I0{200}≦5.0 when I{200} is a result of the X-ray diffraction intensity of {200} crystal plane of sheet surface and I0{200} is a result of the X-ray diffraction intensity of {200} crystal plane of a standard powder of pure copper, and wherein 0.2% yield strength in a rolling parallel direction (RD) is 800 MPa or more and 950 MPa or less, an electrical conductivity of 43.5% IACS or more and 53.0% IACS or less, 180 degree bending workability in a rolling parallel direction (GW) and a rolling perpendicular direction (BW) is R/t=0, and a difference between the rolling parallel direction (RD) and a rolling perpendicular direction (TD) of the 0.2% yield strength is 40 MPa or less.
A method of manufacturing a copper alloy sheet material comprising:
Dependencies are inferred from the claim text.