A process for preparing a water based heat insulating coating composition, said process comprising:
- (a) preparing a graft copolymer emulsion by:
- (i) providing water, an emulsifier, a buffer and a freeze-thaw agent in a reactor maintained at a temperature in the range of 25° C. to 40° C. and speed of agitation in the range of 10 rpm to 50 rpm;
- (ii) heating the reactor to a temperature in the range of 50° C. to 80° C. and adding a hard segment monomer and at least one functional additive to the reactor to obtain a first reaction mixture;
- (iii) adding a polymerization initiator dissolved in water to said first reaction mixture at a feed rate in the range of 2 ml/min to 20 ml/min to initiate polymerization of said hard segment monomer and to obtain a growing hard segment polymer backbone;
- (iv) adding a first reinforcing monomer at a feed rate in the range of 2 ml/min to 20 ml/min to the reactor to initiate grafting of said first reinforcing monomer onto the growing hard segment polymer backbone;
- (v) on complete addition of said first reinforcing monomer, adding a first mixture comprising at least one soft segment monomer and at least one functional additive, at a feed rate in the range of 2 ml/min to 20 ml/min to the reactor and initiating grafting of said soft segment monomer onto the growing hard segment polymer backbone and initiate polymerization of said soft segment monomer to obtain a growing soft segment polymer backbone;
- (vi) on complete addition of said first mixture, adding the first reinforcing monomer at a feed rate in the range of 2 ml/min to 20 ml/min to initiate grafting of the first reinforcing monomer onto the growing soft segment polymer backbone;
- and
- (vii) on complete addition of said first reinforcing monomer in substep (vi), adding a second mixture comprising said second reinforcing additive and at least one functional additive to the reactor to initiate grafting of the second reinforcing monomer onto the backbones of the growing hard segment polymer and growing soft segment polymer and continuing the reactions for a time period in the range of 2 to 6 hours and then cooling to obtain said graft copolymer emulsion;
- (viii) isolating said graft copolymer emulsion from the reactor in a vessel to obtain an isolated graft copolymer emulsion;
- (b) adding a colorant to said isolated graft copolymer emulsion in the vessel while stirring;
- and
- (c) adding at least one reinforcing additive to the vessel after step (b) while stirring to obtain said water based heat insulating coating composition.