A method of producing a sintered sliding material with excellent corrosion resistance, heat resistance, and wear resistance, the method comprising the steps of:
- obtaining a mixed powder by mixing a plurality of powders containing one or more among Cu, Ni, Sn, P, and C in such a way that a total composition of the mixed powder becomes:
- 36-86 mass % of Ni;
- ;
- 1-11 mass % of Sn;
- 0.05-1.0 mass % of P;
- 1-9 mass % of C;
- and the Cu balance by using at least one of:
- a Cu—Ni alloy powder in which a C content is 0.6 mass % or less and a Si content is 0.15 mass % or less as inevitable impurities;
- and a Ni—Cu alloy powder in which a C content is 0.6 mass % or less and a Si content is 0.15 mass % or less as inevitable impurities;
- producing a green compact by pressing the mixed powder;
- and
- obtaining a sintered sliding material having a structure containing:
- an integrated matrix;
- and free graphite dispersed in a plurality of pores by sintering the green compact at 960-1140° C. so that a plurality of grains of alloy made of a Cu—Ni alloy or a Ni—Cu alloy disperse in the plurality of pores in the grain boundaries of the plurality of grains of alloy.