Method, process and fabrication technology for oxide layers
AssigneeSpecmat Limited
InventorsHoria M. Faur, Maria Faur
Life of this patent
Estimating the term…
Abstract
This disclosure relates to a Room Temperature Wet Chemical Growth (RTWCG) method and process of SiOX thin film coatings which can be grown on various substrates. The invention further relates to RTWCG method and process suited to grow thin films on the Si substrates used in the manufacture of silicon-based electronic and photonic (optoelectronic) device applications. The invention further relates to processes used to produce SiOX thin film layers for use as passivation layers, low reflectance layers, or high reflectance single layer coatings (SLARC) and selective emitters (SE).
Claims11
1-37. (canceled)
A method for creating a passivation oxide on silicon, the method comprising the steps of:
- (A) supplying a chemical solution comprising:
- (A1) one or more fluorine-containing acid compounds or fluorine-containing acids;
- (A2) one or more additional compounds selected from one or more of 2,4-dihydroxypiridine, pyridine, dichloropyridazin-3(2H)-one, one or more iodine-containing acids, sulfuric acid, pyridoxine hydrochloride, one or more selenium-containing acid compounds or selenium-containing acids, silver (I) oxide, or silver (II) oxide;
- and
- (A3) water;
- (B) exposing a silicon surface to the solution of Step (A);
- and
- (C) subjecting the silicon to a thermal treatment step comprising:
- (C1) a ramp-up step of about 400 seconds at a temperature of from about 350° C. to about 725° C.;
- (C2) a plateau step of about 300 seconds;
- and
- (C3) a ramp down step to room temperature.
The method of claim 1, wherein component (A1) is hydrofluoric acid.
The method of claim 1, wherein component (A1) is hydrofluoric acid, (A2) is silver (I) oxide and (A3) is water.
The method of claim 1, wherein component (A1) is hydrofluoric acid, (A2) is silver (II) oxide and (A3) is water.
The method of claim 1, wherein component (A1) is hydrofluoric acid, (A2) is one or more selenium-containing acid compounds or selenium-containing acids one or more selenium-containing acid compounds or selenium-containing acids and (A3) is water.
The method of claim 1, wherein the solution is formulated to etch silicon quickly enough to remove an emitter in less than about 80 seconds.
The method of claim 1, wherein the solution is formulated to grow a thin film that passivates the surface after a thermal budget has been applied thereto.
The method of claim 1, wherein the thermal budget of Step (C) is an annealing budget comprising a ramp-up Step (C1) of about 400 seconds at a temperature of from about 350° C. to about 725° C., followed by a plateau Step (C2) of about 300 seconds, then a pre-ramp-down step of about 400 seconds down to a temperature of about 350° C., followed by a ramp down Step (C3) to room temperature.
A structure comprising at least one passivation layer formed using the method of claim 1.
A structure comprising at least one silver-rich layer formed using the method of claim 1.
Dependencies are inferred from the claim text.