Bimodal Propylene Polymers and Sequential Polymerization
AssigneeExxonMobil Chemical Patents Inc.
InventorsLuo Lubin, Matthew W. Holtcamp, Gregory S. Day
Life of this patent
Estimating the term…
Abstract
This invention relates to high porosity (≧15%) and/or low pore diameter (PD<165 μm) propylene polymers and propylene polymerization processes using single site catalyst systems with supports having high surface area (SA≧400 m2/g), low pore volume (PV≦2 mL/g), a specific mean pore diameter range (PD=1-20 nm), and high average particle size (PS≧30 μm).
Claims25
A process to polymerize propylene comprising:
- (a) contacting propylene monomer under polymerization conditions with a catalyst system comprising a single site catalyst precursor compound, an activator, and a support comprising an average particle size of more than 30 μm, a surface area of 400 m2/g or more, a pore volume of from 0.5 to 2 mL/g, and a mean pore diameter of from 1 to 20 nm (10 to 200 Å);
- (b) polymerizing the propylene in (a) for a time period, Al to form a first mode of propylene polymer comprising at least 50 mol % propylene;
- (c) adding hydrogen or other chain transfer agent and optional comonomer to the polymerization after time period A1;
- (d) then polymerizing the propylene in (a) in the presence of at least 1 mmol of the hydrogen or other chain transfer agent per mol of propylene for a time period, A2, wherein a concentration of the hydrogen or other chain transfer agent during time period A2 is greater than the concentration of the hydrogen or other chain transfer agent in time period A1 to form a second mode of the propylene polymer having a lower Mw with respect to the first mode;
- and
- (e) forming a matrix of the propylene polymer, the matrix having a porosity, after time period A2, of 15% or more, as determined by mercury intrusion porosimetry.
3 more elements
A propylene polymer comprising:
- at least 50 mol % propylene;
- a 1% Secant flexural modulus of at least 1000 MPa, determined according to ASTM D 790 (A, 1.0 mm/min);
- more than 5 and less than 200 regio defects per 10,000 propylene units, determined by 13C NMR;
- a multimodal molecular weight distribution;
- if comonomer is present, a CDBI of 50% or more;
- and
- a matrix having a porosity of 15 percent or more, and median pore diameter less than 165 μm, as determined by mercury intrusion porosimetry.
4 more elements