A coated article which is formed by coating a substrate with a powder coating material comprising a fluorinated polymer (A), a polyester polymer (B), an ultraviolet absorber (D) and titanium oxide (E) and which has a cured film of the above powder coating material, wherein
- the thickness of the cured film is from 20 to 1,000 μm,
- when the total of the respective atom number concentrations of C element, O element, F element and Ti element present in a region (I) within 5 μm in depth from the surface of the cured film as obtained by the following method (1) is set to be 100%, the atom number concentration of Ti element is from 0 to 9%,
- when the total of the respective atom number concentrations of C element, O element, F element and Ti element present in a region (II) beyond 10 μm in depth from the surface of the cured film as obtained by the following method (2) is set to be 100%, the atom number concentration of Ti element is from 8.5 to 15%, and
- the proportion of the ultraviolet absorber (D) contained in the above region (I) (100 mass %) as obtained by the following method (3) is from 0.5 to 10 mass %:
- Method (1):
- By observing a cross section of the cured film by a scanning electron microscope equipped with an energy dispersive X-ray analyzer, the respective atom number concentrations of C element, O element, F element and Ti element present in the region (I) are analyzed by the energy dispersive X-ray analyzer, to determine the atom number concentration of Ti element, when the total of the respective atom number concentrations of C element, O element, F element and Ti element is set to be 100%,
- Method (2):
- By observing a cross section of the cured film by a scanning electron microscope equipped with an energy dispersive X-ray analyzer, with respect to the following region (II-1) in a case where the thickness of the cured film is at least 20 μm and less than 30 μm, the following regions (II-1) to (II-2) in a case where the thickness of the cured film is at least 30 μm and less than 40 μm, the following regions (II-1) to (II-3) in a case where the thickness of the cured film is at least 40 μm and less than 50 μm, the following regions (II-1) to (II-4) in a case where the thickness of the cured film is at least 50 μm and less than 60 μm, the following regions (II-1) to (II-5) in a case where the thickness of the cured film is at least 60 μm, the respective atom number concentrations of C element, O element, F element and Ti element present in the respective regions are analyzed by the energy dispersive X-ray analyzer, to determine the atom number concentration of Ti element, when the total of the respective atom number concentrations of C element, O element, F element and Ti element is set to be 100%, in each region, whereupon the atom number concentrations of Ti element in the respective regions are summed up and divided by the number of regions to obtain an average value,
- Region (II-1):
- a region beyond 10 μm and at most 20 μm in depth from the surface of the cured film,
- Region (II-2):
- a region beyond 20 μm and at most 30 μm in depth from the surface of the cured film,
- Region (II-3):
- a region beyond 30 μm and at most 40 μm in depth from the surface of the cured film,
- Region (II-4):
- a region beyond 40 μm and at most 50 μm in depth from the surface of the cured film,
- Region (II-5):
- a region beyond 50 μm and at most 60 μm in depth from the surface of the cured film,
- Method (3):
- By scraping off the region (I) with a cutter, the obtained powder is subjected to high performance liquid chromatography analysis, whereby the amount of the ultraviolet absorber (D) per unit mass in the above powder is obtained from a peak derived from the ultraviolet absorber (D) by using a calibration curve prepared beforehand.