Abstract
The present disclosure relates to catalysts comprising two heterogeneous chromium catalysts for the polymerization of olefins are provided herein. The catalysts, as well as related compositions and methods using the same, may be used to for the production of polyolefins, including for the production of bimodal molecular weight distribution polyolefins, e.g., polyethylene and copolymers of ethylene and 1-hexene.
Claims20
A composition comprising:
- (A) a first catalyst comprising from 0.25-2 wt. % chromium deposited on a first solid oxide component, wherein the first catalyst has a pore volume from 1.0-3.5 mL/g and a surface area from 250-900 m2/g;
- and
- (B) a second catalyst comprising from about 0.25-2 wt. % chromium deposited on a second solid oxide component, wherein the second catalyst has a pore volume from 1.0-2.5 mL solid/g and a surface area from 400-1000 m2/g;
- wherein the first and second catalysts are present a weight ratio from 1:9-9:1, provided that the first catalyst and second catalyst are not the same.
1 more element
A method comprising:
- (A) obtaining a first catalyst, wherein:
- the first catalyst comprising from 0.25-2 wt. % chromium deposited on a first solid oxide component, wherein the first catalyst has a pore volume from 1.0-3.5 mL/g and a surface area from 250-900 m2/g;
- (B) heating the first catalyst to a temperature from 700-900° C. to form an activated first catalyst;
- (C) obtaining a second catalyst, wherein:
- the second catalyst comprising from 0.25-2 wt. % chromium deposited on a second solid oxide component, wherein the second catalyst has a pore volume from 1.0-2.5 mL/g and a surface area from 400-1000 m2/g;
- and
- either one of steps (D) and (E):
- (D) heating the second catalyst to a temperature from 400-700° C. to form an activated second catalyst and then admixing the activated second catalyst to the first activated first catalyst;
- or
- (E) admixing the second catalyst to the activated first catalyst and heating this catalyst mixture to a temperature from 400-700° C. to further activate this catalyst mixture;
- wherein the first and second activated catalysts are present in a weight ratio from 1:9-9:1, provided that the first activated catalyst and second activated catalyst are not the same.
8 more elements