Process and reactor for exothermal reaction
AssigneeHaldor TopsøE A/S
InventorsTroels Dahlgaard STUMMANN, Niels Ulrik ANDERSEN, Madhanakrishnan JANARDHANAN, Jens R. ROSTRUP-NIELSEN
Life of this patent
Estimating the term…
Loading patent…
AssigneeHaldor TopsøE A/S
InventorsTroels Dahlgaard STUMMANN, Niels Ulrik ANDERSEN, Madhanakrishnan JANARDHANAN, Jens R. ROSTRUP-NIELSEN
Estimating the term…
The present disclosure relates to a reactor and a method of operation for an exothermal process being catalyzed by a catalytically active material receiving a reactant gas and providing a product gas, in which said exothermal process has a heat development having a potential for thermally degrading said catalytically active material, and which exothermal process operates at a temperature at which the reactants and at least 80% or all of the products are present as gases, said method comprising the steps of a) directing the reactant gas to a first zone of a material catalytically active in the exothermal process producing an first product gas, and b) directing the first product gas to a second zone of a material catalytically active in the exothermal process producing a product gas, with the option of fully or partially by-passing either said first zone or said second zone, while directing a non-condensing gas stream having a temperature at least 50° C. lower than the product gas to said by-passed zone, wherein the choice of by-passing said zone is made based on the time of operation or a process parameter reflecting the catalytic activity of the zone of catalytically active material which is not by-passed with the associated benefit of reducing the extent of thermal deactivation of the catalytically active material, and thus increasing the overall lifetime of the catalytically active material.
A method of operation for an exothermal process being catalyzed by a catalytically active material comprising a dispersed active metal compound, said process converting a reactant synthesis gas to a product gas, in which the peak temperature of said catalytically active material is at least 40% of the absolute melting temperature of said active metal compound, said method comprising the steps of
A reactor for an exothermal gaseous process having a reactor inlet and a reactor outlet, a first zone of catalytically active material, having a first zone inlet, and having a first zone outlet, a second zone of catalytically active material having a second zone inlet and having a second zone outlet, said reactor being configurable for directing the flow from the reactor inlet to the first zone inlet, directing the flow from the first zone outlet to the second zone inlet, and directing the flow from the second zone outlet to the reactor outlet and said reactor comprising a double blocking-gas valve configured, when said valve is open, for fully or partially by-passing said second zone, where said fully or partially by-passing of said second zone is obtained by directing all, or at least 90%, at least 80% or at least 50% of the flow from the reactor inlet to the first zone inlet, and directing the flow from the first zone outlet through said double blocking-gas valve said reactor outlet or a position downstream said reactor outlet.