Pyrolytic carbon black composite and method of making the same
AssigneeUT-Battelle, LLC
InventorsAmit K. NASKAR, Mariappan Parans PARANTHAMAN
Life of this patent
Estimating the term…
Abstract
A method of recovering carbon black includes the step of providing a carbonaceous source material containing carbon black. The carbonaceous source material is contacted with a sulfonation bath to produce a sulfonated material. The sulfonated material is pyrolyzed to produce a carbon black containing product comprising a glassy carbon matrix phase having carbon black dispersed therein. The pyrolysis can be conducted at a temperature from 1100° C. to 1490° C. A method of making a battery electrode and a lithium ion or sodium ion battery is also disclosed.
Claims50
A method of recovering carbon black, comprising the steps of:
- providing a carbonaceous source material containing carbon black;
- contacting the carbonaceous source material with a sulfonation bath to produce a sulfonated material;
- and,
- pyrolyzing the sulfonated material at a temperature of from 1100 to 1490° C. to produce a layered carbon black containing product comprising a glassy carbon matrix phase having carbon black dispersed therein, the layered carbon black containing product having an interlayer spacing of from 0.4 to 0.5 nm.
A method of making a battery electrode comprising carbon black, the method comprising the steps of:
- providing a carbonaceous source material containing carbon black;
- contacting the carbonaceous source material with an oleum bath to produce a sulfonated material;
- pyrolyzing the sulfonated material at a temperature of from 1100 to 1490° C. to produce a layered carbon black product comprising a glassy carbon matrix phase having carbon black dispersed therein, the layered carbon black containing product having an interlayer spacing of from 4 to 5 angstroms;
- and,
- forming a battery electrode from the carbon black containing product.
A battery, comprising:
- an anode comprising layered carbon black containing product obtained by providing a carbonaceous source material containing carbon black, contacting the carbonaceous source material with an oleum bath to produce a sulfonated material, pyrolyzing the sulfonated material at a temperature of from 1100 to 1490° C. to produce the layered carbon black product comprising a glassy carbon matrix phase having carbon black dispersed therein, the layered carbon black containing product having an interlayer spacing of from 4 to 5 angstroms;
- a cathode;
- and,
- an electrolyte disposed between the anode and the cathode.
Dependencies are inferred from the claim text.