Composite silicon or composite tin particles
OwnerShailesh Upretiinventor
Life of this patent
Estimating the term…
Abstract
The specification relates to a composite particle for storing lithium. The composite particle is used in an electrochemical cell. The composite particle includes a metal oxide on the surface of the composite particle, a major dimension that is approximately less than or equal to 40 microns and a formula of MM′Z, wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co. Zr, K, and Na, and Z is from the group of O, Cl, P, C, S, H, and F.
Claims20
An electrochemical rechargeable cell comprising:
- an anode comprising a particulate composite MM′Z, a binder and a solvent, the MM′Z composite being subtractively removed from an alloy in which M content is not dominant in the alloy and a cooling rate from a melt temperature of the alloy was sufficient to allow a formation of a structure having an extended M phase network and a substantially differentiated phase, the MM′Z composite including a portion of the M′ remaining within the structure, the MM′Z composite further including an amorphous component on the surface of the composite, wherein the structure of MM′Z composite particle possesses rods arranged in an array such that the rods are joined crystallographically and extend into space in a manner providing for a space of separation between crystallite extensions thereby accommodating for volume expansion when storing lithium, and wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co, Zr, K, and Na and Z is from the group of O, Cl, P, C, S, H, and F.
A method of preparing a composite for storing lithium, the method comprising the steps of:
- subtractively removing a MM′Z composite particle from an alloy in which M content is not dominant in the alloy and a cooling rate from a melt temperature of the alloy was sufficient to allow a formation of a structure having an extended M phase network and a substantially differentiated phase, the MM′Z composite particle including a portion of the M′ remaining within the structure, the composite particle further including an amorphous component Z on the surface of the MM′Z composite particle, wherein the structure of MM′Z composite particle possesses rods arranged in an array such that the rods are joined crystallographically and extend into space in a manner providing for a space of separation between crystallite extensions thereby accommodating for volume expansion when storing lithium, and wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co, Zr, K, and Na and Z is from the group of O, Cl, P, C, S, H, and F.
The method as claimed in claim;
- 9 wherein the MM′Z composite particle is at least 80-95% M by weight.
An electrochemical rechargeable cell comprising:
- an anode comprising a particulate composite, a binder and a solvent, the particulate composite having a general formula of MM′Z, wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co, Zr, K, and Na, and Z is from the group of O, Cl, P, C, S, H, and F, the particulate composite having a surface composition being an oxide, the surface composition being textured, and wherein a major dimension of the particle is less than 100 microns, and wherein at least 2% by weight of M′ is doped into a crystal structure of M, and wherein M is arranged in an array of columns joined by crystallographic alignments with separation between the columns.
Dependencies are inferred from the claim text.