Selective laser sintering method, heat treatment method, metal powder, and shaped product
AssigneeJapan Silicolloy Industry Co., Ltd.
InventorTakayasu Shimizu
Life of this patent
Estimating the term…
Abstract
A selective laser sintering method alternately repeats a step of forming silicon alloy A2 powder (metal powder) in layers, the silicon alloy A2 powder made of high silicon stainless steel containing C:less than 0.10, Si:2.0˜9.0, Mn:0.05˜6.0, Cu:0.5˜4.0, Ni:1.0˜24.0, Cr:6.0˜28.0, Mo:0.2˜4.0, Nb:0.03˜2.0 in wt % and the balance of Fe and inevitable impurities, and a step of selectively applying a laser to the silicon alloy A2 powder formed in layers to melt and sinter the silicon alloy A2 powder.
Claims11
A selective laser sintering method comprising:
- alternately repeating
- a step of forming metal powder in layers, the metal powder being made of high silicon stainless steel containing C:less than 0.10, Si:2.0˜9.0, Mn:0.05˜6.0, Cu:0.5˜4.0, Ni:1.0˜24.0, Cr:6.0˜28.0, Mo:0.2˜4.0, Nb:0.03˜2.0 in wt %, and a balance of Fe and inevitable impurities;
- and
- a step of selectively applying a laser to the metal powder formed in layers to melt and sinter the metal powder.
Metal powder used in a selective laser sintering method that selectively applies a laser to metal powder to melt and sinter the metal powder for lamination, wherein
- the metal powder is made of high silicon stainless steel containing C:less than 0.10, Si:2.0˜9.0, Mn:0.05˜6.0, Cu:0.5˜4.0, Ni:1.0˜24.0, Cr:6.0˜28.0, Mo:0.2˜4.0, Nb:0.03˜2.0 in wt %, and a balance of Fe and inevitable impurities.
Dependencies are inferred from the claim text.