Transparent glass-ceramic articles, glass-ceramic precursor glasses and methods for forming the same
AssigneeCorning Incorporated
InventorsGeorge Halsey Beall, Charlene Marie Smith, Steven Alvin Tietje
Life of this patent
Estimating the term…
Abstract
Embodiments of glass ceramic articles and precursor glasses are disclosed. In one or more embodiments, the glass-ceramic articles are transparent and include a nepheline phase and a phosphate phase. The glass-ceramic articles are colorless and exhibit a transmittance of about 70% or greater across the visible spectrum. The glass-ceramic articles may optionally include a lithium aluminosilicate phase. The crystals of the glass-ceramic articles may have a major cross-section of about 100 nm or less.
Claims24
A device comprising:
- a glass-ceramic article comprising:
- a major nepheline phase;
- and
- a minor phosphate phase,
- wherein the glass-ceramic article is colorless and has transmission or reflection color coordinates under the CIE L*, a*, b* colorimetry system of L* in the range from about 80 to about 100, a* in the range from about −5 to about 5, and b* in the range from about b* in the range from about −5 to about 5, and exhibits a transmittance of about 70% or greater across the visible spectrum, in the range from about 390 nm to about 700 nm,
- wherein the device comprises any one of an electronic device, an automotive application, an architectural applications and an energy production application.
A glass comprising a composition, in mol %, comprising:
- SiO2 in the range from about 35 to about 60,
- Al2O3 in the range from about 10 to about 30,
- Na2O in the range from about 7 to about 31,
- K2O in the range from about 0 to about 20,
- Li2O in the range from about 0 to about 20,
- P2O5 in the range from about 1.5 to about 8, and
- a rare earth oxide in the range from about 0 to about 6.
A method of forming a glass ceramic comprising:
- heat treating a precursor glass article by heating the at a rate in the range from about 1° C./minute to about 10° C./minute to a temperature in the range from about 600° to about 1000° C.;
- and cooling the glass-ceramic article to about room temperature,
- wherein heating treating the precursor glass article comprises any one or more of:
- a) heating the precursor glass article to a nucleating temperature (Tn) in the range from about 700° C. to about 900° C.,
- b) maintaining the precursor glass article at the Tn to produce a nucleated precursor glass article,
- c) heating the nucleated precursor glass article at a rate in the range from about 1° C./minute to about 10° C./minute to a crystallization temperature (Tc) in the range from about 600° to about 1000° C., and
- d) maintaining the nucleated precursor glass article at the Tc to produce a glass-ceramic article having a nepheline crystalline phase.
Dependencies are inferred from the claim text.