Back to results
US 2016/0235886 A1Published application
Wet-pack intraocular lens materials with high refractive index
AssigneeNovartis AG
InventorsXuwei Jiang, Douglas Schlueter, Walter Laredo
Life of this patent
Estimating the term…
Abstract
Intraocular lens materials are disclosed. They are soft and very deformable and have a high refractive index, and a high glistening resistance in fully hydrated state. They are particularly suitable for making wet-packed intraocular lenses (IOLs) which can be delivered through sub 2.0 mm incisions.
Claims20
A polymeric intraocular lens material, which is polymerization product of a polymerizable composition comprising
- (a) from about 10% to about 30% by weight of a hydrophilic monomer relative to the total amount of all polymerizable components, wherein the hydrophilic monomer is hydroxyethylmethacrylate, hydroxyethylacrylate, N-hydroxyethylmethacrylamide, N-hydroxyethylacrylamide, N,N-dimethylacrylamide, N,N-dimethylmethacrylamide, or a combination thereof,
- (b) from about 20% to about 85% by weight of one or more poly(phenyl ether)-containing monomers of formula (I) relative to the total amount of all polymerizable components
- wherein:
- R1 is H or CH3;
- Ra, Rb, Rc, Rd, Re, Rf, Rg, Rh, and Ri independent of one another are H, C1-C12 alkyl, or C1-C12 alkoxy;
- Bp is a direct bond, (CH2)m1, or (OCH2CH2)m2, in which m1 is 2-6 and m2 is 1-10;
- n1 is an integer from 1 to 9;
- n2 is an integer from 0 to 6;
- Yp is a direct bond, O, S, OC(═O)NH, NHC(═O)NH, or NR′ in which R′ is H, C1-C10 alkyl, C6H5, or CH2C6H5,
- (c) from 0 to about 50% by weight of one or more aryl acrylic monomers of formula (II) relative to the total amount of all polymerizable components
- wherein A1 is H or CH3;
- B1 is (CH2)m1 or [O(CH2)2]Z1 in which m1 is 2-6 and z1 is 1-10;
- Y1 is a direct bond, O, S, or NR′ in which R′ is H, CH3, Cn′H2n′+1 in which n′=1-10, iso-OC3H7, C6H5, or CH2C6H5;
- W1 is 0-6, provided that m1+w1≦8;
- and D1 is H, Cl, Br, C1-C4 alkyl, C1-C4 alkoxy, C6H5, or CH2C6H5, and
- (d) one or more polymerizable crosslinking agents,
- wherein the listed components and any additional polymerizable components add up to 100% by weight,
- wherein the intraocular lens material in a fully-hydrated state has:
- a glass transition temperature of less than 22° C., a refractive index of 1.55 or greater measured at 589 nm and at room temperature (23±2° C.), an equilibrium water content of less than 5.0% by weight at a temperature of from 16° C. to 45° C., a Young's modulus of less than 80 MPa, an elongation of at least 100%, a 100% secant modulus of less than 6.0 MPa, and a glistening resistance characterized by having no bright field microvacuoles and about 10 or less microvacuoles per viewing screen.
16 more elements
Dependencies are inferred from the claim text.