Bearing steel having improved fatigue durability and method of manufacturing the same
AssigneeHyundai Motor Company
InventorsSung-Chul CHA, Si-Yup LEE, Young-Sang KO, Moon-Ki BAE, Seung-Hyun HONG
Life of this patent
Estimating the term…
Abstract
A bearing steel includes 1.0 to 1.3 wt % carbon; 0.9 to 1.6 wt % silicon; 0.5 to 1.0 wt % manganese; 1.5 to 2.5 wt % nickel; 1.5 to 2.5 wt % chromium; 0.2 to 0.5 wt % molybdenum; 0.01 to 0.06 wt % aluminum; 0.01 to 0.1 wt % copper; at least one selected from the group consisting of more than 0 wt % and less than 0.38 wt % vanadium and more than 0 wt % and less than 0.02 wt % niobium; and a balance of iron.
Claims7
A bearing steel comprising:
- based on a total weight of the bearing steel,
- 1.0 to 1.3 wt % carbon;
- 0.9 to 1.6 wt % silicon;
- 0.5 to 1.0 wt % manganese;
- 1.5 to 2.5 wt % nickel;
- 1.5 to 2.5 wt % chromium;
- 0.2 to 0.5 wt % molybdenum;
- 0.01 to 0.06 wt % aluminum;
- 0.01 to 0.1 wt % copper;
- at least one selected from the group consisting of more than 0 wt % and less than 0.38 wt % vanadium and more than 0 wt % and less than 0.02 wt % niobium;
- and
- a balance of iron.
9 more elements
A method of manufacturing a bearing steel, comprising steps of:
- primarily spheroidizing a wire rod of an alloy comprising:
- based on a total weight of the bearing steel,
- 1.0 to 1.3 wt % carbon;
- 0.9 to 1.6 wt % silicon;
- 0.5 to 1.0 wt % manganese;
- 1.5 to 2.5 wt % nickel;
- 1.5 to 2.5 wt % chromium;
- 0.2 to 0.5 wt % molybdenum;
- 0.01 to 0.06 wt % aluminum;
- 0.01 to 0.1 wt % copper;
- at least one selected from the group consisting of more than 0 wt % and less than 0.38 wt % of vanadium and more than 0 wt % and less than 0.02 wt % of niobium;
- and
- a balance of iron at 720 to 850° C. for 4 to 8 hours;
- wire-drawing the primarily spheroidized wire rod;
- secondarily spheroidizing the wire-drawn wire rod at 720 to 850° C. for 4 to 8 hours;
- forging the secondarily spheroidized wire rod to form the bearing steel;
- and
- quenching, rapidly cooling, and tempering the bearing steel.
15 more elements