METHOD FOR PRODUCING JOURNAL PART OF 9 TO 12% Cr STEEL TURBINE ROTOR, AND JOURNAL PART PRODUCED BY THE METHOD
AssigneeJapan Casting & Forging Corporation
InventorsYoshihiro Okamura, Yasushi Wakeshima
Life of this patent
Estimating the term…
Loading patent…
AssigneeJapan Casting & Forging Corporation
InventorsYoshihiro Okamura, Yasushi Wakeshima
Estimating the term…
In a journal part of a 9 to 12 wt % Cr steel turbine rotor, a groove face is formed, and on the groove face, a lower build-up layer is formed by using a first welding material containing C: 0.10 to 0.25 wt %, Si: 0.20 to 0.80 wt %, Mn: 1.0 to 2.5 wt %, Ni: 0.4 to 1.0 wt %, Cr: 1.0 to 3.0 wt %, Mo: 0.2 to 1.5 wt %, V: 0.03 to 0.10 wt %, and a remainder composed of Fe and inevitable impurities, and further on this lower build-up layer, an upper build-up layer is formed using a second welding material containing C: 0.10 to 0.25 wt %, Si: 0.20 to 0.80 wt %, Mn: 1.0 to 2.5 wt %, Ni: 0.4 to 1.0 wt %, Cr: 1.0 to 3.0 wt %, Mo: 0.2 to 1.5 wt %, and a remainder consisting of Fe and inevitable impurities.
A method for producing a 9 to 12 wt % Cr steel turbine rotor comprising:
Dependencies are inferred from the claim text.