High-carbon hot-rolled steel sheet and method for manufacturing the same
AssigneeJfe Steel Corporation
InventorsYuka MIYAMOTO, Takashi KOBAYASHI, Chikara KAMI
Life of this patent
Estimating the term…
Abstract
There is provided a high-carbon hot-rolled steel sheet and method for producing the same. The steel sheet has excellent hardenability consistently, even when annealed in a nitrogen atmosphere, and excellent workability. The steel sheet has a hardness in the range of 65 or less in terms of HRB and a total elongation El of 40% or more before a quenching treatment is performed.
Claims8
A high-carbon hot-rolled steel sheet, the steel sheet having a chemical composition comprising:
- C:
- 0.20% or more and 0.48% or less, by mass %;
- Si:
- 0.10% or less, by mass %;
- Mn:
- 0.50% or less, by mass %;
- P:
- 0.03% or less, by mass %;
- S:
- 0.010% or less, by mass %;
- acid-soluble Al:
- 0.10% or less, by mass %;
- N:
- 0.0050% or less, by mass %;
- B:
- 0.0005% or more and 0.0050% or less, by mass %;
- one or more elements selected from Sb, Sn, Bi, Ge, Te, and Se such that the total content of the one or more elements is in the range of 0.002% or more and 0.030% or less, by mass %;
- and
- Fe and incidental impurities,
- wherein the high-carbon hot-rolled steel sheet has (i) a microstructure including ferrite and cementite, a density of the cementite in the ferrite grains being in the range of 0.10 pieces/μm2 or less, (ii) a hardness in the range of 65 or less in terms of HRB, and (iii) a total elongation in the range of 40% or more.
A method for manufacturing a high-Carbon hot-roiled steel sheet, the method comprising:
- performing hot rough rolling on a steel sheet having a chemical composition comprising:
- C:
- 0.20% or more and 0.48% or less by mass %;
- Si:
- 0.10% or less, by mass %;
- Mn:
- 0.50% or less, by mass %;
- P:
- 0.03% or less, by mass %;
- S:
- 0.00% or less, by mass %;
- acid-soluble Al:
- 0.10% or less, by mass %;
- N:
- 0.0050% or less, by mass %;
- B:
- 0.0050% or more and 0.0050% or less, by mass %;
- one or more elements selected from Sb, Sn, Bi, Ge, Te, and Se such that the total content of the one or more elements is in the range of 0.002% or more and 0.030% or less, by mass %;
- and
- Fe and incidental impurities;
- thereafter performing finish rolling with a finishing temperature in the range of the Ar3 transformation temperature or higher;
- coiling the hot-rolled steel sheet at a coiling temperature in the range of 500° C. to 750° C.;
- thereafter heating and holding the coiled steel sheet at a temperature equal to the Ac1 transformation temperature or higher for a holding time in the range of 0.5 hours or more;
- cooling the heated steel sheet to a temperature lower than the Ar1 transformation temperature at a cooling rate in the range of 1° C./h or more and 20° C./h or less;
- and
- holding the steel sheet at a temperature lower than the Ar1 transformation temperature for a period in the range of 20 hours or more.
A method for manufacturing a high-carbon hot-rolled steel sheet, the method comprising:
- performing hot rough rolling on a steel sheet having a chemical composition comprising:
- C:
- 0.20% or more and 0.48% or less, by mass %;
- Si:
- 0.10% or less, by mass %;
- Mn:
- 0.50% or less, by mass %;
- P:
- 0.03% or less, by mass %;
- S:
- 0.010% or less, by mass %;
- acid-soluble Al:
- 0.10% or less, by mass %;
- N:
- 0.0050% or less, by mass %;
- B:
- 0.0005% or more and 0.0050% or less, by mass %;
- one or more elements selected from Sb, Sn, Bi, Ge, Te, and Se such that the total content of the one or more elements is in the range of 0.002% or more and 0.030% or less, by mass %;
- at least one element selected from Ni, Cr, and Mo such that the total content of the at least one element is in the range of 0.50% or less;
- and
- Fe and incidental impurities;
- thereafter performing finish rolling with a finishing temperature equal to the Ar3 transformation temperature or higher;
- coiling the hot-roiled steel sheet at a coiling temperature in the range of 500° C. to 750° C.;
- thereafter heating and holding the coiled steel sheet at a temperature in the range of the Ac1 transformation temperature or higher for a holding time in the range of 0.5 hours or more;
- cooling the heated steel sheet to a temperature lower than the Ar1 transformation temperature at a cooling rate in the range of 1° C./h or more and 20° C./h or less;
- and
- holding the steel sheet at a temperature lower than the Ar1 transformation temperature for a period in the range of 20 hours or more.
Dependencies are inferred from the claim text.