Thick, high-strength, sour-resistant line pipe and method for producing same
AssigneeJfe Steel Corporation
InventorsAkihiko Tanizawa, Haruo Nakamichi, Toru Kawanaka, Noriaki Uchitomi, Takafumi Ozeki
Life of this patent
Estimating the term…
Loading patent…
AssigneeJfe Steel Corporation
InventorsAkihiko Tanizawa, Haruo Nakamichi, Toru Kawanaka, Noriaki Uchitomi, Takafumi Ozeki
Estimating the term…
A line pipe having a wall thickness of 20 mm or more and a tensile strength of 560 MPa or more and a production method therefor are provided. The base metal portion contains particular amounts of C, Si, Mn, P, S, Al, Nb, Ca, N, and O, one or more component selected from Cu, Ni, Cr, Mo, V, and Ti as optional components, and the balance being Fe and unavoidable impurities. The microstructure in the pipe thickness direction contains 90% or more bainite and 1% or less of MA in a region that extends from a position 2 mm from an inner surface to a position 2 mm from an outer surface. In a hardness distribution in the pipe thickness direction, the hardness in a region other than a center segregation area is 220 Hv10 or less and the hardness in the center segregation area is 250 Hv10 or less. The major axes of pores, inclusions, and inclusion clusters that are present in a portion that extends from, a position 1 mm from the inner surface to a 3/16 position of the tube thickness and in a portion that extends from a position 1 mm from the outer surface to a 13/16 position of the tube thickness in the tube thickness direction are 1.5 mm or less.
A heavy wall, high-strength line pipe for sour gas service, wherein a chemical composition of a steel pipe base metal portion contains, in terms of % by mass, C:
A method for producing a heavy wall, high-strength line pipe for sour gas service, the method comprising reheating a continuously cast slab having the chemical composition according to claim 1 to 1000 to 1150° C.;
A method for producing a heavy wall, high-strength line pipe for sour gas service, the method comprising reheating a continuously cast slab having the chemical composition according to claims 2 to 1000 to 1150° C.;
Dependencies are inferred from the claim text.