Methods and compositions for a low temperature operating solid oxide fuel cell (SOFC) are provided. The SOFC includes a Sr0.8La0.2TiO3 (SLT) support layer, a (La0.9Sr0.1)0.98(Ga0.8Mg0.2)O3-δ (LSGM) electrolyte layer and□a cathode layer disposed on top of said electrolyte layer.
Claims20
A low temperature operating solid oxide fuel cell (SOFC), comprising:
- a Sr0.8La0.2TiO3 (SLT) support layer;□
- a (La0.9Sr0.1)0.98(Ga0.8Mg0.2)O3-δ (LSGM) electrolyte layer;
- and□
- a cathode layer disposed on top of said electrolyte layer.
1 more element
A method of making a solid oxide fuel cell, comprising:
- preparing an SLT powder via solid state reaction using SrCO3, La2O3, and TiO2 precursors to form a calcinated SLT product;□
- dispersing the calcinated SLT powder with graphite and poly(vinylbutyral) (PVB) to form a homogeneous mixture;
- drying the homogenous mixture to form a dried product;
- pressing the dried product using a die;
- and
- bisque firing the pressed product.
3 more elements
A low temperature operating solid oxide fuel cell (SOFC), comprising:
- a Sr0.8La0.2TiO3 (SLT) support layer;□
- a (La0.9Sr0.1)0.98(Ga0.8Mg0.2)O3-δ (LSGM) electrolyte layer;
- and□
- a cathode layer disposed on top of said electrolyte layer,
- wherein the SLT support layer and LSGM electrolyte layer comprise a laminated, tape-casted ceramic structure.