Antimony based anode material for rechargeable batteries and preparation method
AssigneeBelenos Clean Power Holding AG
InventorsMaksym V. KOVALENKO, He MENG, Kostiantyn KRAVCHYK, Marc WALTER
Life of this patent
Estimating the term…
Loading patent…
AssigneeBelenos Clean Power Holding AG
InventorsMaksym V. KOVALENKO, He MENG, Kostiantyn KRAVCHYK, Marc WALTER
Estimating the term…
An antimony based anode material for a rechargeable battery comprises nanoparticles of composition SbMxOy where M is a further element selected from the group consisting of Sn, Ni, Cu, In, Al, Ge, Pb, Bi, Fe, Co, Ga, with 0≦x<2 and 0≦y≦2.5+2x. The nanoparticles form a substantially monodisperse ensemble with an average size not exceeding a value of 30 nm and by a size deviation not exceeding 15%. A method for preparing the antimony based anode material is carried out in situ in a non-aqueous solvent and starts by reacting an antimony salt and an organometallic amide reactant and oleylamine.
An antimony based anode material for a rechargeable battery, the anode material comprising nanoparticles of composition SbMxOy where M is a further element selected from the group consisting of Sn, Ni, Cu, In, Al, Ge, Pb, Bi, Fe, Co, Ga, with 0≦x<2 and 0≦y≦2.5+2x, wherein the nanoparticles form a substantially monodisperse ensemble with an average size between 5 nm and 30 nm and a size deviation not exceeding 15%.
A method for preparing an antimony based anode material which comprises nanoparticles of composition SbMxOy where M is a further element selected from the group consisting of Sn, Ni, Cu, In, Al, Ge, Pb, Bi, Fe, Co, Ga, with 0≦x<2 and 0≦y≦2.5+2x, wherein the nanoparticles form a substantially monodisperse ensemble with an average size between 5 nm and 30 nm and a size deviation not exceeding 15%, wherein said method comprises the steps of:
A rechargeable battery comprising an anode and a cathode, wherein the anode comprises an antimony based anode material which comprises nanoparticles of composition SbMxOy where M is a further element selected from the group consisting of Sn, Ni, Cu, In, Al, Ge, Pb, Bi, Fe, Co, Ga, with 0≦x<2 and 0≦y≦2.5+2x, wherein the nanoparticles form a substantially monodisperse ensemble with an average size between 5 nm and 30 nm and a size deviation not exceeding 15%.