[Problem] To increase adhesive strength between an aqueous base coat layer and a clear coat layer in a coating method by a two-coat one-bake system where an aqueous base coat paint is coated, then a clear coat paint is coated, and these two coated films are simultaneously hardened, in comparison with the conventional method. [Solution] Provided is a coating method using a specific hardener in a clear coat paint. Namely, the hardener is characterized in that (1) it includes a reaction product of (i) a derivative of 1,6-hexamethylene diisocyanate including a trimer and virtually not including a diisocyanate monomer, and (ii) a compound having both an active hydrogen and a hydrophilic group; and (2) viscosity at 23° C. is not more than 1,000 mPa·s. The compound having both an active hydrogen and a hydrophilic group herein is a compound having an active hydrogen-containing group and a sulfo group represented by formula (I), and preferably the sulfo group in a hardener is neutralized with a tertiary amine. X—R—SO3H Formula (I) (in the formula, X is an amino group, alkylamino group, cycloalkylamino group, or hydroxyl group, R is an aliphatic and/or alicyclic hydrocarbon group.)
-7. (canceled)
A coating method comprising applying an aqueous base coat paint, without hardening the aqueous base coat paint by cross-linking, subsequently coating a clear coat paint comprising a hardener and an active hydrogen-containing resin on the base coat paint, hardening the base coat paint and the clear coat paint simultaneously by cross-linking, wherein the clear coat paint is a two-component polyurethane paint with a mole ratio of 0.9 to 2.0 in NCO/H (active hydrogen), wherein
Dependencies are inferred from the claim text.