Higher Strength, Mullite-Based Iron Foundry Filter
AssigneePorvair PLC
InventorRudolph A. Olson, III
Life of this patent
Estimating the term…
Abstract
A ceramic foam filter and method of making the filter is described. The filter comprises: a sintered reaction product of: 35-75 wt % aluminosilicate; 10-30 wt % colloidal silica; 0-2 wt % bentonite; and 0-35 wt % fused silica; wherein the ceramic foam filter has less than 0.15 wt % alkali metals measured as the oxide and a flexural strength of at least 60 psi measured at 4 minutes at 1428° C.
Claims28
A ceramic foam filter comprising:
- a sintered reaction product of:
- 35-75 wt % aluminosilicate;
- 10-30 wt % colloidal silica;
- 0-2 wt % bentonite;
- 0-35 wt % fused silica;
- and
- 0-10 wt % pore formers;
- wherein said ceramic foam filter has less than 0.15 wt % alkali metals measured as the oxide.
12-21. (canceled)
A ceramic foam filter comprising:
- a sintered reaction product of:
- 35-75 wt % aluminosilicate;
- 10-30 wt % colloidal silica;
- 0-2 wt % bentonite;
- and
- 0-35 wt % fused silica;
- wherein said ceramic foam filter has less than 0.15 wt % alkali metals measured as the oxide and a flexural strength of at least 60 psi measured at 4 minutes at 1428° C.
23-31. (canceled)
A process for forming a ceramic foam filter comprising the steps of:
- preparing a ceramic precursor comprising:
- 35-75 wt % aluminosilicate;
- 10-30 wt % colloidal silica;
- 0-2 wt % bentonite;
- 0-35 wt % fused silica;
- 0-10 wt % pore formers;
- and
- solvent in balance;
- impregnating an organic foam with said ceramic precursor;
- heating said impregnated organic foam to a temperature sufficient to volatize said organic foam and sinter said ceramic precursor thereby forming said ceramic foam filter;
- wherein said ceramic foam filter has less than 0.15 wt % alkali metals measured as the oxide.
A process for forming a ceramic foam filter comprising the steps of:
- preparing a ceramic precursor comprising:
- 35-75 wt % aluminosilicate;
- 10-30 wt % colloidal silica;
- 0-2 wt % bentoniate;
- 0-35 wt % fused silica;
- 0-10 wt % pore formers;
- and
- solvent in balance;
- impregnating an organic foam with said ceramic precursor;
- heating said impregnated organic foam to a temperature sufficient to volatize said organic foam and sinter said ceramic precursor thereby forming said ceramic foam filter;
- wherein said ceramic foam filter has a flexural strength of at least 60 psi measured at 4 minutes at 1428° C.