Abstract
In a steel sheet having a specific chemical composition and having a microstructure including ferrite that is a soft first phase by 20-50% in terms of the area ratio, the remainder being tempered martensite and/or tempered bainite that is a hard second phase, the microstructure of steel of a surface layer section of the steel sheet from the surface to the depth of 100 μm and a center section of t/4-3t/4 (t is the sheet thickness) is controlled.
Claims5
A cold-rolled steel sheet, comprising:
- C:
- 0.05-0.30 mass %;
- Si:
- 3.0 mass % or less, (exclusive of 0) mass %;
- Mn:
- 0.1-5.0 mass %;
- P:
- 0.1 mass % or less, (exclusive of 0) mass %;
- S:
- 0.02 mass % or less, (exclusive of 0) mass %;
- Al:
- 0.01-1.0 mass %;
- and
- N:
- 0.01 mass % or less, (exclusive of 0) mass % respectively;
- iron and inevitable impurities,
- wherein
- a microstructure comprises ferrite that is a soft first phase by 20-50% in terms of area ratio, and tempered martensite, tempered bainite, or both, that is a hard second phase;
- a difference between area ratio Vαs of ferrite of a steel sheet surface layer section from a steel sheet surface to a depth of 100 μm and area ratio Vαc of ferrite of a center section of t/4-3t/4 ΔVα=Vαs−Vαc is less than 10%, where t is a sheet thickness;
- and
- a ratio of hardness Hvs of the steel sheet surface layer section and hardness Hvc of the center section RHv=Hvs/Hvc is 0.75-1.0.
A cold-rolled steel sheet comprising:
- C:
- 0.05-0.30 mass %;
- Si:
- 3.0 mass % or less, (exclusive of 0) mass %;
- Mn:
- 0.1-5.0 mass %;
- P:
- 0.1 mass % or less, (exclusive of 0) mass %;
- S:
- 0.02 mass % or less, (exclusive of 0) mass %;
- Al:
- 0.01-1.0 mass %;
- and
- N:
- 0.01 mass % or less, (exclusive of 0) mass % respectively iron and inevitable impurities, wherein
- a microstructure comprises ferrite that is a soft first phase by 20-50% in terms of area ratio, and tempered martensite, tempered bainite, or both, that is a hard second phase;
- a difference between area ratio Vαs of ferrite of a steel sheet surface layer section from a steel sheet surface to a depth of 100 μm and area ratio Vαc of ferrite of a center section of t/4-3t/4 ΔVα=Vαs−Vαc is 10-50%, where t is a sheet thickness;
- and
- an average grain size of ferrite of the steel sheet surface layer section is 10 μm or less.
Dependencies are inferred from the claim text.