High-Strength Aluminum Alloy Brazing Sheet And Method Of Manufacture
AssigneeUacj Corporation
InventorsMakoto Ando, Akio Niikura, Yoichiro Bekki
Life of this patent
Estimating the term…
Abstract
An aluminum alloy brazing sheet having a core material of an aluminum alloy, and a filler material cladded on the core is disclosed. The core material is an aluminum alloy having about 0.05 to about 1.2 mass Si, about 0.05-about 1.0 mass % Fe, about 0.05-about 1.2 mass % Cu, and about 0.6-about 1.8 mass % Mn, balance Al and the inevitable impurities. The, filler material includes an aluminum alloy having about 2.5-about 13.0 mass % Si. Also, there is provided a method of manufacturing such an aluminum alloy brazing sheet.
Claims10
A method of manufacturing a high strength aluminum alloy brazing sheet comprising:
- casting an aluminum alloy of a core material and a filler material at a casting speed to provide a cast core material and a cast filler material, respectively;
- combining the cast core material with the cast filler material so that the cast filler material is cladded to at least one surface of the cast core material to produce a composite material;
- a heating process wherein the composite material is heated and held after the combining process to form a heat treated composite material;
- and
- hot clad rolling the heat treated composite material,
- wherein the casting speed V (mm/min) and an amount of cooling water W (kg/min×cm) applied during the casting satisfy formula (1) in the casting process for said core material:
- 25≦0.4×V+W (1);
- wherein the composite material is held at a temperature within a range of about 400° C. to about 500° C. over a time period of 0 hrs to about 10 hrs during the heating process;
- wherein the time period for the hot clad rolling which is counted from start of the hot clad rolling to the time taken to reduce an initial thickness of the composite material by 50 mm is at most 5 min,
- wherein the temperature of the composite material falls within a range of about 400° C. to about 450° C. when the thickness of said composite material is reduced by 50 mm;
- wherein a time period counted from the time when the thickness of the composite material is reduced by 50 mm to the time taken to reduce the thickness of the composite material to 20 mm is at most 10 min,
- wherein the temperature of the composite material is about 300° C. to about 400° C. when the thickness of the composite material is reduced to 20 mm;
- wherein a time period which is counted from the rolling start to a rolling end is at most 40 min, and
- wherein the aluminum alloy comprises a core material comprising an aluminum alloy;
- and a filler material cladded on at least one surface of the core material and comprising an Al/Si-based alloy, wherein the core material is an aluminum alloy which contains Si within a range of about 0.05 mass % to about 1.2 mass %, Fe within a range of about 0.05 mass % to about 1.0 mass %, Cu within a range of about 0.05 mass % to about 1.2 mass %, and Mn within a range of about 0.6 mass % to about 1.8 mass %, and which comprises as balance Al and inevitable impurities;
- wherein the filler material is an aluminum alloy which contains Si falling within a range of about 2.5 mass % to about 13.0 mass %, and Fe falling within a range of about 0.05 mass % to about 1.0 mass %, and comprises as balance Al and inevitable impurities;
- wherein an area percentage is occupied with intermetallic compounds having a size falling within a range of about 0.2 μm to about 0.5 μm is at most 5%;
- and wherein a solid solution amount of Mn is at least 0.2 mass % in the core.
A method of manufacturing a high strength aluminum alloy brazing sheet comprising:
- casting an aluminum alloy of a core material, a filler material and a sacrificial anode material, respectively, at a casting speed to provide a cast core material, a cast filler material and a cast sacrificial anode material, respectively;
- combining the cast core material with the cast filler material and the cast sacrificial anode material whereby the cast filler material is cladded to at least one surface of the cast core material and whereby the cast sacrificial anode material is applied to another surface of the cast core material to produce a composite material;
- a heating process wherein the composite material is heated and held after the combining process to form a heat treated composite material;
- and
- hot clad rolling the heat treated composite material,
- wherein the casting speed V (mm/min) and an amount of cooling water W (kg/min×cm) applied during the casting formula (1) while the core material:
- 25≦0.4×V+W (1);
- wherein the composite material is held at a temperature within a range of about 400° C. to about 500° C. over a time period of 0 to about 10 hrs during the heating;
- and
- wherein the time period for the hot clad rolling which is counted from start of the hot clad rolling to the time taken to reduce an initial thickness of the composite material by 50 mm is at most 5 min;
- and
- wherein the temperature of said composite material is about 400° C. to about 450° C. when the thickness of said composite material is reduced by 50 mm;
- and
- wherein the time period counted from the time when the thickness of the composite material is reduced by 50 mm to the time taken to reduce the thickness of the composite material to 20 mm is at most 10 min;
- and
- and wherein a temperature of the composite material is about 300° C. to about 400° C. when the thickness of the composite material is reduced to 20 mm;
- and
- wherein a time period counted from the rolling start to a rolling end is up to 40 min, and
- wherein the aluminum brazing sheet comprises a core material comprised of an aluminum alloy;
- a filler material cladded on one surface of said core material and comprised of an Al/Si-based alloy;
- and a sacrificial anode material cladded on another surface of the core material and comprised of an aluminum alloy,
- wherein the core material is an aluminum alloy having Si within a range of about 0.05 mass % to about 1.2 mass %, Fe within a range of about 0.05 mass % to about 1.0 mass %, Cu within a range of about 0.05 mass % to about 1.2 mass %, and Mn within a range of about 0.6 mass % to about 1.8 mass %, and balance Al and inevitable impurities;
- wherein the filler material is an aluminum alloy having Si within a range of about 2.5 mass % to about 13.0 mass %, and Fe within a range of about 0.05 mass % to about 1.0 mass %, balance Al and inevitable impurities;
- wherein the sacrificial anode material is an aluminum alloy having Zn within a range of about 0.5 mass % to about 6.0 mass %, Si within a range of about 0.05 mass % to about 1.5 mass %, and Fe within a range of about 0.05 mass % to about 2.0 mass %, and balance Al and inevitable impurities;
- wherein an area percentage is occupied with intermetallic compounds having a size within a range of 0.2 μm to 0.5 μm is at most 5%;
- and wherein a solid solution amount of Mn is at least 0.2 mass % in the core material.
Dependencies are inferred from the claim text.