Aqua Regia and Hydrogen Peroxide HCl Combination to Remove Ni and NiPt Residues
AssigneesIntermolecular, Inc., Globalfoundries Inc.
InventorsAnh Duong, Clemens Fitz, Olov Karlsson
Life of this patent
Estimating the term…
Abstract
A method for cleaning residues from a semiconductor substrate during a nickel platinum silicidation process is disclosed, including a multi-step residue cleaning, including exposing the substrate to an aqua regia solution, followed by an exposure to a solution having hydrochloric acid and hydrogen peroxide. The SC2 solution can further react with remaining platinum residues, rendering it more soluble in an aqueous solution and thereby dissolving it from the surface of the substrate.
Claims17
A formulation for processing nickel platinum, the formulation comprising:
- water;
- nitric acid mixed with the water;
- and
- a non-chlorine based acid mixed with the water and the nitric acid,
- wherein a concentration of the nitric acid in the formulation is less than about 15 wt %.
A formulation for processing nickel platinum, the formulation comprising:
- water;
- hydrogen peroxide mixed with the water;
- and
- hydrochloric acid mixed with the water and the hydrogen peroxide,
- wherein a concentration of the hydrogen peroxide in the formulation is less than or equal to about 25 wt %.
A formulation for processing nickel platinum, the formulation comprising:
- water;
- nitric acid mixed with the water;
- and
- hydrochloric acid mixed with the water and the nitric acid,
- wherein a concentration of the nitric acid in the formulation is less than about 15 wt % and a concentration of the hydrochloric acid in the formulation is less than about 20 wt %.
Dependencies are inferred from the claim text.