US 2015/0104629 A1Published application
Gypsum wallboard produced using a high water-to-stucco ratio
AssigneeUnited States Gypsum Company
InventorsBangji CAO, Weixin D. SONG, Cesar CHAN
Life of this patent
Estimating the term…
Abstract
A gypsum composition, board, and method of producing a gypsum board with increased fire endurance are described. The set gypsum-containing composition can be used to prepare a gypsum board having fire endurance, based on particular water-to-stucco ratios.
Claims20
A fire resistant gypsum board comprising:
- a set gypsum composition disposed between two cover sheets, the set gypsum composition comprising an interlocking matrix of set gypsum formed from a slurry comprising at least stucco and water;
- the slurry having a water-to-stucco ratio from about 0.7 to about 2.0;
- and
- the board having a density from about 24 lbs/ft3 to about 40 lbs/ft3, and when at a thickness of about ⅝ inch, a nail pull resistance of at least about 70 lbs of force as determined according to ASTM C473-09, and a Fire Endurance Index (FEI) greater than about 52 minutes.
1 more element
A fire resistant gypsum board comprising:
- a set gypsum composition disposed between two cover sheets, the set gypsum composition comprising an interlocking matrix of set gypsum formed from a slurry comprising at least stucco and water;
- the slurry having a water-to-stucco ratio from about 1.2 to about 2.0;
- the board having a density from about 24 lbs/ft3 to about 40 lbs/ft3, and when at a thickness of about % inch, a nail pull resistance of at least about 70 lbs of force as determined according to ASTM C473-09, and a Fire Endurance Index (FEI) greater than about 54 minutes.
A method for making a fire resistant gypsum board comprising:
- forming a mixture of at least stucco and water,
- disposing the slurry on a first sheet,
- disposing a second sheet on the slurry to form a board preform having two cover sheets,
- cutting the board preform into a board of predetermined dimensions after the slurry has hardened sufficiently for cutting, and
- drying the board;
- the slurry having a water-to-stucco ratio from about 0.7 to about 2.0;
- the board when dried having a density from about 24 lbs/ft3 to about 40 lbs/ft3, and when at a thickness of about % inch, a nail pull resistance of at least about 70 lbs of force as determined according to ASTM C473-09, and a Fire Endurance Index (FEI) greater than about 52 minutes.
4 more elements
Dependencies are inferred from the claim text.