Steel wire material and method for manufacturing same
AssigneeKabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsMikako TAKEDA, Shohei Nakakubo, Kazuhiko Kirihara, Masayuki Endo
Life of this patent
Estimating the term…
Loading patent…
AssigneeKabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsMikako TAKEDA, Shohei Nakakubo, Kazuhiko Kirihara, Masayuki Endo
Estimating the term…
A method of manufacturing a steel wire material that contains 0.05%-1.2% C (“%” means “% by mass,” same hereinafter for chemical components.), 0.01%-0.7% Si, 0.1%-1.5% Mn, 0.02% max. P (not including 0%), 0.02% max. S (not including 0%), and 0.005% max. N (not including 0%), with the remainder being iron and unavoidable impurities. The steel wire material has a scale 6.0-20 μm thick and holes of an equivalent circle diameter of 1 μm max. in said scale that occupy 10% by area max. Said scale does not detach in the cooling process after hot rolling or during storage or transportation but can readily detach during mechanical descaling.
A method for manufacturing a steel wire material comprising:
Dependencies are inferred from the claim text.