Method of Manufacturing a Stiff Engineered Composite
OwnerGavin R. McIntyre, Jeffrey D. Betts +2inventors
InventorsGavin R. McIntyre, Jeffrey D. Betts, Gregory Tudryn, Liam Mooney
Life of this patent
Estimating the term…
Abstract
The method of making a compressed biocomposite body includes compressing a mass of biocomposite material comprised of discrete particles and a network of interconnected glucan-containing mycelia cells in the presence of heat and moisture into a compressed body having a density in excess of 18 pcf. Compression may take place batch wise in a press or continuously in a path of narrowing cross-section defined by a series of heated rollers.
Claims28
A method of making a composite body comprising the steps of
- obtaining a mass of biocomposite material comprised of discrete particles, a network of interconnected glucan-containing mycelia cells extending around the discrete particles and a moisture content of from 45% to 70%;
- placing the biocomposite material in a compression fixture;
- heating the biocomposite material in the compression fixture while compressing the biocomposite material into a compressed body of a desired density and shape within said compression fixture;
- maintaining the compressed body under heat and compression for a time sufficient to allow cross-linking between the glucans in said mycelia cells to bind the discrete particles together in the compressed body;
- removing the compressed body from the compression fixture;
- and
- heating the removed compressed body to dehydrate the compressed body to reduce said moisture content to less than 30% and to deactivate the mycelia cells.
A method of making a composite body comprising the steps of
- obtaining a mass of biocomposite material comprised of discrete particles, a network of interconnected glucan-containing mycelia cells extending around the discrete particles and a moisture content of greater than 10% by weight;
- molding said mass into a plurality of tiles of rectangular shape;
- stacking said tiles in alternating manner with a plurality of wooden veneers and with a plate of porous plastic on an underside thereof to from a stack;
- compressing said stack to compress said tiles to approximately three times density while drying the compressed tiles to obtain a pre-compressed biocomposite body;
- thereafter compressing said pre-compressed biocomposite body at a force of 20 tons and at a temperature of 600° F. for a time of two minutes while reducing the moisture content to less than 10% to obtain a compressed composite body.
A method of making a composite body comprising the steps of
- obtaining a mass of biocomposite material comprised of discrete particles, a network of interconnected glucan-containing mycelia cells extending around the discrete particles and a moisture content of greater than 10% by weight;
- and
- thereafter compressing said mass at a pressure between 25 psi and 5000 psi and at a temperature of 600° F. for a time of four minutes while reducing the moisture content to less than 10% to obtain a compressed composite body.
A method of making a composite body comprising the steps of
- obtaining a mass of biocomposite material comprised of discrete particles, a network of interconnected glucan-containing mycelia cells extending around the discrete particles and a moisture content of greater than 10% by weight;
- and
- thereafter compressing said mass at a pressure between 25 psi and 5000 psi and at a temperature of 300° F. for a time of one minute while reducing the moisture content to less than 10% to obtain a compressed composite body.
A method of making a composite body comprising the steps of
- obtaining a mass of biocomposite material comprised of discrete particles, a network of interconnected glucan-containing mycelia cells extending around the discrete particles and a moisture content of greater than 10% by weight;
- forming said mass of biocomposite material into a flat blank board of 1.25″ thickness with a 0.25″ hemp nonwoven matt grown into at least one face of said flat blank board;
- thereafter compressing said flat blank board into the predetermined curved shape under a compressive force of 3000 psi and at a temperature of 340° F. for a time of 10 minutes while reducing the moisture content to less than 10% to obtain a compressed composite body of curved shape.
A method of making a composite body comprising the steps of
- cultivating mycelium into a sheet;
- freeze drying said sheet;
- thereafter milling said dried sheet to form a first mass of particles;
- milling Kenaf pith to form a second mass of particles;
- blending said first mass of particles and said second mass of particles into a mixture;
- thereafter heating and compressing said mixture in a mold cavity for a time sufficient to form a cohesive product;
- and
- removing said product from the mold as a self-supporting composite body.
A self-supporting composite body comprising a substrate of discrete particles and a network of interconnected mycelia cells extending through and around the discrete particles and bonding the discrete particles together, said composite body being characterized in being stiff and in having a density between 18 and 60 pounds per cubic foot (pcf), a modulus of elasticity of up to 250 ksi and a modulus of rupture of up to 2500 psi.
A self-supporting composite body comprising a substrate of discrete fibers and a network of interconnected mycelia cells extending through and around the discrete fibers and bonding the discrete fibers together, said composite body being characterized in being stiff and in having a density between 18 and 60 pounds per cubic foot (pcf), a modulus of elasticity greater than 250 ksi and a modulus of rupture of up to 2500 psi.
Dependencies are inferred from the claim text.