Cathode materials for lithium battery having higher performance
AssigneeLG Chem, Ltd.
InventorsJens M. Paulsen, Hong-Kyu Park, Sun Sik Shin, Sinyoung Park, Hyeyun Cha
Life of this patent
Estimating the term…
Loading patent…
AssigneeLG Chem, Ltd.
InventorsJens M. Paulsen, Hong-Kyu Park, Sun Sik Shin, Sinyoung Park, Hyeyun Cha
Estimating the term…
Provided is a method for preparing the heat-treated mixture of an oxide powder (a) represented by Formula I and an oxide powder (b) represented by Formula II, LiCoO2 (I) LizMO2 (II) wherein 0.95<z<1.1; M=Ni1-x-yMnxCoy, 0<y<0.5, and a ratio of Mn to Ni (x/(1-x-y)) is in the range of 0.4 to 1.1, comprising mixing (i) a Co-containing precursor, (ii) an Mn—Ni-containing precursor, and (iii) optionally, an Li-containing precursor, and heat-treating the mixture at a temperature of more than 400° C. under an oxygen-containing atmosphere.
A method for preparing the heat-treated mixture of an oxide powder (a) represented by Formula I and an oxide powder (b) represented by Formula II, wherein a mixing ratio of the oxide powder (a):oxide powder (b) is in the range of 30:70 to 90:10, the oxide powder (a) is monolithic particles having a D50 of more than 10 μm, and the oxide powder (b) is agglomerated particles having a D50 of less than 10 μm, and heat treatment is carried out at a temperature of 400° C. or higher:
Dependencies are inferred from the claim text.