A positive electrode for a secondary battery, which is used to manufacture a lithium ion secondary battery, characterized in that:
- the positive electrode is composed of:
- a positive electrode current collector;
- and
- a positive electrode electroactive substance layer that is comprised of a positive electrode electroactive substance, a conductive auxiliary, and a binder, which is coated at least on one surface of the positive electrode current collector,
- wherein
- the positive electrode electroactive substance is
- a lithium containing complex oxide comprising cobalt or nickel, or
- a combination of a spinel type lithium-manganese complex oxide represented by LiMn2O4 or the like and a lithium-nickel complex oxide represented by LixNiyAlzCowO2;
- wherein the content ratio of the spinel type lithium-manganese complex oxide to the lithium-nickel complex oxide, which are comprised in the combination;
- (the mass of the spinel type lithium-manganese complex oxide/the mass of the lithium-nickel complex oxide) is selected within the range of no larger than 80/20;
- the positive electrode is produced by forming the positive electrode electroactive substance layer through following step 1 to step 5:
- (Step 1)
- a step of preparing a positive electrode mixture by mixing the positive electrode electroactive substance, the conductive agent, and the binding agent in a humidity atmosphere at a relative humidity of 10% to a relative humidity of 70%;
- (Step 2)
- a step of preparing a positive electrode mixture coating liquid (pasty slurry) by dispersing the positive electrode mixture in an organic solvent that is used as a dispersion solvent;
- (Step 3)
- a step of forming a positive electrode mixture coating liquid layer by coating the positive electrode mixture coating liquid on the positive electrode current collector;
- (Step 4)
- a step of drying the positive electrode mixture coating liquid layer to provide a dried positive electrode mixture coating liquid layer;
- and
- (Step 5)
- a step of compression-molding the dried positive electrode mixture coating liquid layer to form the positive electrode electroactive substance layer;
- wherein the condition used for drying the positive electrode mixture coating liquid layer in the step 4 is selected either of following two drying condition:
- “drying condition” in which heating to a temperature selected in the range of 100° C. to 160° C. is performed under unreduced pressure, or
- “drying condition” in which heating to a temperature selected in the range of 80° C. to 130° C. is performed in a vacuum of 0.1 Pa to 100 Pa;
- a concentration of chemically adsorbed water based on a total mass W3 of the positive electrode electroactive substance, which is comprised in the positive electrode electroactive substance layer of the positive electrode that is subjected to the treatment of drying under the selected condition for drying the positive electrode mixture coating liquid layer in the step 4, is selected within the range of 0.06% by mass to 0.3% by mass, wherein
- the chemically adsorbed water is water content that is to be detected in a range of 200° C. to 300° C. by Karl Fischer titration method.