Method for obtaining extreme selectivity of metal nitrides and metal oxides
AssigneeMicron Technology, Inc.
InventorKevin R. Shea
Life of this patent
Estimating the term…
Abstract
Methods for etching metal nitrides and metal oxides include using ultradilute HF solutions and buffered, low-pH HF solutions containing a minimal amount of the hydrofluoric acid species H2F2. The etchant can be used to selectively remove metal nitride layers relative to doped or undoped oxides, tungsten, polysilicon, and titanium nitride. A method is provided for producing an isolated capacitor, which can be used in a dynamic random access memory cell array, on a substrate using sacrificial layers selectively removed to expose outer surfaces of the bottom electrode.
Claims19
A method of selectively etching a layer of metal nitrides or metal oxide, the method comprising:
- heating a substrate having formed thereon a structure comprising a layer of metal oxide or metal nitride;
- exposing the structure to a buffered hydrofluoric acid etch solution having a pH between about 3.5 and about 5.5;
- and
- selectively etching the layer of metal oxide or metal nitride with an etch rate selectivity relative to an exposed layer of silicon greater than or equal to about 2000:1.
A method of selectively removing a sacrificial material, the method comprising:
- providing a structure which includes a sacrificial material comprising a metal oxide or a metal nitride and further includes a nonsacrificial material;
- exposing the structure to a buffered hydrofluoric acid solution having a pH between about 3.5 and 5.5 and heated to a temperature between about 50° C. and about 90° C.;
- and
- selectively removing the sacrificial material from the structure with an etch rate selectivity relative to the nonsacrificial material greater than about 500:1.
A method of selectively removing a sacrificial material, the method comprising:
- providing a structure comprising a sacrificial material and a nonsacrificial material, the sacrificial material comprising a metal oxide or a metal nitride;
- exposing the structure to a buffered hydrofluoric acid solution having a buffer to hydrofluoric acid ratio exceeding about 400:1;
- and
- selectively removing the sacrificial material from the structure with an etch rate selectivity relative to the nonsacrificial material exceeding about 500:1.
Dependencies are inferred from the claim text.