Back to results
US 2014/0272665 A1Published application
Ceramic Fuel Cell With Enhanced Flatness And Strength And Methods Of Making Same
AssigneesRedox Power Systems, LLC, University of Maryland, College Park
InventorsHee Sung YOON, Eric D. WACHSMAN, Bryan M. BLACKBURN
Life of this patent
Estimating the term…
Abstract
Ceramic fuel cells having enhanced flatness and strength are disclosed. The fuel cell can include a half-cell having, in order, a patterned layer, an anode support layer and an electrolyte layer. Methods of making ceramic fuel cells are also provided.
Claims124
A ceramic fuel cell comprising, in order:
- a sintered patterned layer having a first coefficient of thermal expansion;
- a sintered anode support layer having a second coefficient of thermal expansion;
- a sintered first electrolyte layer having a third coefficient of thermal expansion;
- and
- a cathode layer,
- wherein the second coefficient of thermal expansion is not between the first coefficient of thermal expansion and the third coefficient of thermal expansion.
3 more elements
A method of making a ceramic fuel cell comprising:
- providing a first structure comprising, in order:
- a patterned layer comprising, prior to sintering, green bodies having a first composition;
- an anode support layer comprising, prior to sintering, green bodies having a second composition;
- and
- a first electrolyte layer comprising, prior to sintering, green bodies having a third composition;
- sintering the first structure at a first sintering temperature to obtain a second structure comprising, in order:
- a sintered patterned layer;
- a sintered anode support layer;
- and
- a sintered first electrolyte layer;
- wherein the sintered patterned layer has a first coefficient of thermal expansion, the sintered anode support layer has a second coefficient of thermal expansion, and the sintered first electrolyte layer has a third coefficient of thermal expansion;
- the second coefficient of thermal expansion is not between the first coefficient of thermal expansion and the third coefficient of thermal expansion.
9 more elements
A method of making a ceramic fuel cell comprising:
- providing a first structure comprising, in order:
- a patterned layer comprising, prior to sintering, green bodies having a first composition;
- an anode support layer comprising, prior to sintering, green bodies having a second composition;
- and
- a first electrolyte layer comprising, prior to sintering, green bodies having a third composition;
- sintering the first structure at a first sintering temperature to obtain a second structure comprising, in order:
- a sintered patterned layer;
- a sintered anode support layer;
- and
- a sintered first electrolyte layer;
- wherein, during sintering, the first composition has a first shrinkage, the second composition has a second shrinkage, and the third composition has a third shrinkage;
- and
- the second shrinkage is not between the first shrinkage and the third shrinkage.
10 more elements
A ceramic fuel cell comprising:
- a second structure comprising, in order:
- a sintered patterned layer;
- a sintered anode support layer;
- and
- a sintered first electrolyte layer;
- wherein the second structure is obtained by the process of:
- providing a first structure comprising, in order:
- a patterned layer comprising, prior to sintering, green bodies having a first composition;
- an anode support layer comprising, prior to sintering, green bodies having a second composition;
- and
- a first electrolyte layer comprising, prior to sintering, green bodies having a third composition;
- sintering the first structure at a first sintering temperature;
- wherein, during sintering, the first composition has a first shrinkage, the second composition has a second shrinkage, and the third composition has a third shrinkage;
- and
- the second shrinkage is not between the first shrinkage and the third shrinkage.