Compositions and methods for manufacturing sol-gel derived bioactive borophosphate glasses for medical applications
OwnerGregory J. Pomrink, Zehra Tosun +2inventors
InventorsGregory J. Pomrink, Zehra Tosun, Cecilia Cao, Roy Layne Howell
Life of this patent
Estimating the term…
Abstract
A sol-gel bioactive glass precursor, method for making sol-gel glasses, resultant sol-gel bioactive glasses, and methods of use thereof which include at least 5 weight percent CaO, at least 10 weight percent P2O5, at least 10 weight percent Na2O, and at least 25 weight percent B2O3, wherein the bioactive glass is substantially silica-free. Medical and industrial uses of such glasses.
Claims34
A sol-gel derived bioactive glass composition, wherein the bioactive glass is at least 5 weight percent CaO, at least 10 weight percent P2O5, at least 10 weight percent Na2O, and at least 25 weight percent B2O3, wherein the bioactive glass is substantially silica-free.
A sol-gel bioactive glass precursor including a source of Ca, P, Na, and B wherein the sol-gel bioactive glass precursor is substantially Si free.
A method of making a sol-gel bioactive glass, wherein the bioactive glass is at least 5 weight percent CaO, at least 10 weight percent P2O5, at least 10 weight percent Na2O, and at least 25 weight percent B2O3, wherein the bioactive glass is substantially silica-free comprising:
- mixing a sol-gel bioactive glass precursor including a source of B, Ca, P, and Na;
- aging the mixture, and;
- drying the mixture to form the sol-gel bioactive glass.
A sol-gel derived bioactive glass composition, wherein the bioactive glass is at least 5 weight percent alkaline earth metal, at least 10 weight percent P2O5, at least 10 weight percent alkali metal, and at least 25 weight percent B2O3, wherein the bioactive glass is substantially silica-free.
A method of making a sol-gel bioactive glass including Si, Ca, P, and Na comprising:
- mixing a sol-gel bioactive glass precursor including a source of Si, Ca, P, and Na, wherein the sodium source is selected from the group consisting of NaCl and C2H5ONa, and;
- drying the mixture at a temperature of 100° C. or lower.
A method of making a sol-gel bioactive glass, wherein the bioactive glass is at least 5 weight percent CaO, at least 5 weight percent P2O5, at least 10 weight percent Na2O, and at least 25 weight percent B2O3, wherein the bioactive glass is substantially silica-free comprising:
- mixing a sol-gel bioactive glass precursor including a source of B, Ca, P, and Na;
- aging the mixture, and;
- drying the mixture to form the sol-gel bioactive glass.
Dependencies are inferred from the claim text.