Method of patterning a low-k dielectric film
AssigneeApplied Materials, Inc.
InventorsChia-Ling Kao, Sean S. Kang, Srinivas D. Nemani
Life of this patent
Estimating the term…
Abstract
Methods of patterning low-k dielectric films are described. In an example, In an embodiment, a method of patterning a low-k dielectric film involves forming and patterning a metal nitride mask layer above a low-k dielectric layer. The low-k dielectric layer is disposed above a substrate. The method also involves passivating the metal nitride mask layer by treating with a plasma based on O2/N2/SixFy. The method also involves etching a portion of the low-k dielectric layer.
Claims20
A method of patterning a low-k dielectric film, the method comprising:
- forming and patterning a metal nitride mask layer above a low-k dielectric layer, the low-k dielectric layer disposed above a substrate;
- passivating the metal nitride mask layer by treating with a plasma based on O2/N2/SixFy;
- and
- etching a portion of the low-k dielectric layer.
A method of patterning a low-k dielectric film, the method comprising:
- forming and patterning a metal nitride mask layer above a low-k dielectric layer, the low-k dielectric layer disposed above a substrate, wherein patterning the metal nitride layer comprises plasma etching performed at a pressure of approximately 40 mTorr, a source power (Ws) of approximately 200 W, a chemistry based on CF4, C4F8, N2 and Ar, at a showerhead to wafer gap of approximately 1.6 mm, for a duration of approximately 30 seconds;
- passivating the metal nitride mask layer by treating with a plasma process performed at a pressure of approximately 20 mTorr, a source power (Ws) of approximately 150 W, a chemistry based on SiF4, N2, O2 and Ar, at a showerhead to wafer gap of approximately 1.25 mm, for a duration of approximately 220 seconds;
- and
- etching a portion of the low-k dielectric layer, wherein the etching comprises plasma etching performed at a pressure of approximately 40 mTorr, a source power (Ws) of approximately 200 W, a chemistry based on SiF4, C4F8, N2 and Ar, at a showerhead to wafer gap of approximately 1.6 mm, for a duration of approximately 85 seconds.
A method of patterning a low-k dielectric film, the method comprising:
- forming and patterning a metal nitride mask layer above a low-k dielectric layer, the low-k dielectric layer disposed above a substrate;
- passivating the metal nitride mask layer by treating with a plasma based on O2/N2/SixFy;
- etching a portion of the low-k dielectric layer;
- repeating the passivating and etching to form trenches having sidewalls in the low-k dielectric layer;
- and
- subsequent to repeating the passivating and etching to form the trenches, passivating the metal nitride mask layer and the sidewalls of the trenches formed in the low-k dielectric layer by treating with a plasma based on O2/N2/SixFy, wherein the passivating comprises depositing a protecting material layer on the metal nitride layer and on the sidewalls of the trenches formed in the low-k dielectric layer;
- and
- etching to extend the trenches in the low-k dielectric layer.
Dependencies are inferred from the claim text.