Accelerated aging of phosphorus-doped optical fibers
AssigneeOFS Fitel, LLC
InventorsDavid John DiGiovanni, Robert L. Lingle, Michael J. LuValle, George E. Oulundsen, Durgesh Vaidya
Life of this patent
Estimating the term…
Abstract
Adverse hydrogen aging limitations in multiply-doped optical fibers are overcome by passivating these optical fibers using a deuterium passivation process. This treatment essentially pre-reacts the glass with deuterium so that the most active glass sites are no longer available to react with hydrogen in service. Optical fibers of main interest are doped with mixtures of germanium and phosphorus. Optimum passivating process conditions are described.
Claims18
A method for passivation of optical fibers, the method comprising:
- applying a first passivation step to an optical fiber, the first passivation step being in an environment comprising deuterium, the first passivation step being at a first pressure, the first passivation step being at a first temperature, the first passivation step being for a first period of time;
- applying a first operation step to the optical fiber, the first operation step being in an atmosphere comprising hydrogen, the first operation step being at a second pressure, the first operation step being at a second temperature, the first operation step being for a second period of time, the first passivation step and the first operation step resulting in a first loss-time curve, the first loss-time curve having a first loss associated with the first loss-time curve;
- applying a second passivation step to the optical fiber, the second passivation step being in the environment comprising deuterium, the second passivation step being at a third pressure, the second passivation step being at a third temperature, the third temperature being greater than the first temperature, the second passivation step being for a third period of time, the second passivation step resulting in a second loss-time curve, the second loss-time curve having a second loss associated with the second loss-time curve, the second passivation step being such that the first loss is less than the second loss;
- and
- applying a second operation step to the optical fiber, the second operation step being in the atmosphere comprising hydrogen, the second operation step being at a fourth pressure, the second operation step being at a fourth temperature, the second operation step being applied for a fourth period of time.
A method for passivation of optical fibers, the method comprising:
- applying a first passivation step to an optical fiber, the first passivation step being in an environment comprising deuterium, the first passivation step being at a first pressure, the first passivation step being at a first temperature, the first temperature being between approximately 65 degrees Celsius and approximately 100 degrees Celsius, the first passivation step being for a first period of time;
- heating the optical fiber in an environment comprising an inert gas;
- applying a first operation step to the optical fiber, the first operation step being in an atmosphere comprising hydrogen, the first operation step being at a second pressure, the first operation step being at a second temperature, the first operation step being for a second period of time, the first passivation step and the first operation step resulting in a first loss-time curve, the first loss-time curve having a first loss associated with the first loss-time curve;
- applying a second passivation step to the optical fiber, the second passivation step being in the environment comprising deuterium, the second passivation step being at a third pressure, the second passivation step being at a third temperature, the third temperature being greater than the first temperature, the second passivation step being for a third period of time, the second passivation step resulting in a second loss-time curve, the second loss-time curve having a second loss associated with the second loss-time curve;
- applying a second operation step to the optical fiber, the second operation step being in the atmosphere comprising hydrogen, the second operation step being at a fourth pressure, the second operation step being at a fourth temperature, the second operation step being for a fourth period of time, the second operation step being such that the first loss is less than the second loss.
A method for passivation of optical fibers, the method comprising:
- applying a first passivation step to the optical fiber, the first passivation step being in an environment comprising deuterium, the first passivation step being at a first pressure, the first pressure being between approximately 0.2 atmospheres of deuterium and approximately 0.6 atmospheres of deuterium, the first passivation step being at a first temperature, the first temperature being between approximately 65 degrees Celsius and approximately 100 degrees Celsius, the first passivation step being for a first period of time;
- heating the optical fiber in an environment comprising an inert gas;
- applying a first operation step to the optical fiber, the first operation step being in an atmosphere comprising hydrogen, the first operation step being at a second pressure, the first operation step being at a second temperature, the first operation step being for a second period of time, the first passivation step and the first operation step resulting in a first loss-time curve, the first loss-time curve having a first loss associated with the first loss-time curve;
- applying a second passivation step to the optical fiber, the second passivation step being in the environment comprising deuterium, the second passivation step being at a third pressure, the second passivation step being at a third temperature, the third temperature being greater than the first temperature, the second passivation step being for a third period of time, the second passivation step resulting in a second loss-time curve, the second loss-time curve having a second loss associated with the second loss-time curve;
- applying a second operation step to the optical fiber, the second operation step being in the atmosphere comprising hydrogen, the second operation step being at a fourth pressure, the second operation step being at a fourth temperature, the second operation step being for a fourth period of time, the second operation step being such that the first loss is less than the second loss;
- comparing the first loss-time curve to a third loss-time curve, the third loss-time curve having a third loss associated with the third loss-time curve, the third loss-time curve being derived from applying a third passivation step to the optical fiber, the third passivation step being in the environment comprising deuterium, the third passivation step being at a fifth pressure, the third passivation step being at a fifth temperature, the third passivation step being for a fifth period of time, the fifth temperature being less than the first temperature;
- and
- applying a third operation step to the optical fiber, the third operation step being in the atmosphere comprising hydrogen, the third operation step being at a sixth pressure, the third operation step being at a sixth temperature, the third operation step being such that the first loss is less than the third loss.
Dependencies are inferred from the claim text.