Back to results
US 2013/0284736 A1Published application
Housing and method for making same
AssigneesFIH (Hong Kong) Limited, Shenzhen Futaihong Precision Industry Co., Ltd.
InventorsShu-Xiang ZHOU, Qiu-Jiang XU, He-Xian LIN
Life of this patent
Estimating the term…
Abstract
A housing includes a plastic substrate, an active layer formed on the plastic substrate, and an exterior layer formed on the active layer. The active layer contains polysiloxane and cetyl trimethyl ammonium bromide. The exterior layer contains silicon dioxide or titanium dioxide, and cetyl trimethyl ammonium bromide.
Claims15
A method for making a housing, comprising:
- providing a plastic substrate;
- forming an activator by mixing silane coupling agent, organic solvent, deionized water, and a leveling agent, the mass ratio of the silane coupling agent, organic solvent, deionized water, and leveling agent being (3-5):(85-92):(3-5):(5-10);
- coating the activator on the surface of the plastic substrate and drying to form an active layer;
- Forming a coating solution by mixing silicon ester or titanium ester, organic solvent, deionized water, and a leveling agent, the mass ratio of the silicon ester or titanium ester, organic solvent, deionized water, and leveling agent being (45-55):(35-45):(3-5):(3-5);
- and
- coating the surface of the active layer with the coating solution and drying the coating solution to form an exterior layer.
3 more elements
A housing, comprising:
- a plastic substrate;
- an active layer formed on the plastic substrate;
- and
- an exterior layer formed on the active layer;
- wherein the active layer contains polysiloxane and cetyl trimethyl ammonium bromide, the exterior layer contains silicon dioxide or titanium dioxide, and cetyl trimethyl ammonium bromide.
2 more elements
Dependencies are inferred from the claim text.