Halogen-Free Resin Composition And Method For Fabricating Halogen-Free Copper Clad Laminate Using The Same
AssigneeGuangdong Shengyi Sci. Tech Co., Ltd.
InventorsYueshan He, Shiguo Su
Life of this patent
Estimating the term…
Loading patent…
AssigneeGuangdong Shengyi Sci. Tech Co., Ltd.
InventorsYueshan He, Shiguo Su
Estimating the term…
The present invention relate to a halogen-free resin composition and a method for fabricating a halogen-free copper clad laminate using the same. The halogen-free resin composition comprises the following components: reactive small molecular polyphenylene oxide with a number average molecular weight of 500-3000, a polybenzoxazine resin, a phosphorus-containing epoxy resin, a composite curing agent, a curing promoter, a filler, and a benzene or ketone solvent. The method for fabricating a halogen-free copper clad laminate comprises: Step 1: dissolving reactive small molecular polyphenylene oxide with a number average molecular weight of 500-3000 in a benzene or ketone solvent, adding a polybenzoxazine resin after dissolution, and mixing by stirring, to prepare a solution for use; Step 2: adding a phosphorus-containing epoxy resin, a composite curing agent, a curing promoter, and a filler to the solution for use, and stirring uniformly, to obtain a colloidal solution; Step 3: evenly coating the prepared colloidal solution to E-glass cloth with an even surface and baking, to produce a B-stage partially cured prepreg; and Step 4: cutting the B-stage partially cured prepreg into a suitable size according to the size of a compressor, precisely overlaying, placing a copper foil on and under the laminated B-stage partially cured Prepregs, and pressing in a vacuum hot pressing machine, to obtain a halogen-free copper clad laminate.
A halogen-free resin composition, comprising from 5 to 30 parts by weight of reactive small molecular polyphenylene oxide with a number average molecular weight of 500-3000, from 5 to 50 parts by weight of a polybenzoxazine resin, from 15 to 65 parts by weight of a phosphorus-containing epoxy resin, from 1 to 25 parts by weight of a composite curing agent, from 0 to 5 parts by weight of a curing promoter, from 0 to 100 parts by weight of a filler, and a suitable amount of benzene or ketone solvent.
Dependencies are inferred from the claim text.