A method of manufacturing a steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness, the method comprising:
- finish hot rolling a steel slab including 0.2 wt % to 0.35 wt % of carbon (C), 0.1 wt % to 0.5 wt % of silicon (Si), 0.5 wt % to 1.8 wt % of manganese (Mn), 0.1 wt % to 0.6 wt % of nickel (Ni), 0.005 wt % to 0.05 wt % of niobium (Nb), 0.005 wt % to 0.02 wt % of titanium (Ti), 0.03 wt % or less of phosphorous (P), 0.03 wt % or less of sulfur (S), 0.05 wt % or less (excluding 0 wt %) of aluminum (Al), 0.01 wt % or less (excluding 0 wt %) of nitrogen (N), and iron (Fe) as well as other unavoidable impurities as a remainder at a residual reduction rate of 50% or more and a temperature ranging from Ar3 to Ar3+200° C.;
- and
- then cooling at a cooling rate ranging from 0.2° C./sec to 4° C./sec.