US 2013/0281625 A1Published application
Methods and Apparatus for Forming Blends of Polyolefin and Resin Modifier
AssigneeExxonMobile Chemicals Patents Inc.
InventorsJay K. Keung, Yann Devorest, Chia Yung Cheng
Life of this patent
Estimating the term…
Abstract
A process for preparing a blend of thermoplastic polymer and resin modifier within a single-screw extruder, wherein the resin modifier is a hydrocarbon resin.
Claims22
A process for preparing a blend of thermoplastic polymer and resin modifier, the process comprising the steps of:
- (i) charging neat thermoplastic polymer to a single-screw extruder;
- (ii) charging neat resin modifier to the extruder;
- (iii) conveying the polyolefin and resin modifier through a feed section of the extruder to form a blend, where the feed section has an average channel depth;
- (iv) conveying the blend through a compression section of the extruder to thereby form a molten blend;
- (v) mixing the molten blend after said step of conveying the blend through the compression section to thereby impart positive pressure on the molten blend in a downstream direction;
- (vi) conveying the molten blend through a metering section, where the metering section has an average channel depth;
- and
- (vii) extruding the molten blend, wherein the blend or molten blend is subjected to a compression ratio that is at least 1.2, where the compression ratio is the ratio of the feed section average channel depth to the metering section average channel depth.
5 more elements
A process for preparing a blend of thermoplastic polymer and resin modifier, the process comprising the steps of:
- (i) charging neat polyolefin to a single-screw extruder;
- (ii) charging neat resin modifier to the extruder wherein the resin modifier is selected from the group consisting of hydrogenated cycloaliphatic resins, and aromatic modified cycloaliphatic hydrocarbon resins or mixtures thereof;
- (iii) conveying the polyolefin and resin modifier through a feed section of the extruder to form a blend, where the feed section has a feed depth;
- (iv) conveying the blend through a compression section of the extruder to thereby form a molten blend;
- (v) mixing the molten blend after said step of conveying the blend through the compression section to thereby impart positive pressure on the molten blend in a downstream direction;
- (vi) conveying the molten blend through a metering section, where the metering section has a metering depth;
- and
- (vii) extruding the molten blend, where during at least one of said step of conveying through a feed section, said step of conveying through a compression section, and said step of conveying through a metering section, the blend or molten blend is subjected to a pressure imparted a compression ratio that is at least 1.2, where the compression ratio is the ratio of the feed depth to the metering depth.
5 more elements
A process for preparing a blend of thermoplastic polymer and resin modifier, the process comprising the steps of:
- (i) charging neat thermoplastic polymer to a single-screw extruder;
- (ii) charging neat resin modifier to the extruder wherein the resin modifier comprises a polycyclopentadiene resin;
- (iii) conveying the thermoplastic polymer and resin modifier through a feed section of the extruder to form a blend, where the feed section has a feed depth;
- (iv) conveying the blend through a compression section of the extruder to thereby form a molten blend;
- (v) mixing the molten blend after said step of conveying the blend through the compression section to thereby impart positive pressure on the molten blend in a downstream direction;
- (vi) conveying the molten blend through a metering section, where the metering section has metering depth;
- and
- (vii) extruding the molten blend, where during at least one of said step of conveying through a feed section, said step of conveying through a compression section, and said step of conveying through a metering section, the blend or molten blend is subjected to a pressure imparted a compression ratio that is at least 1.2, where the compression ratio is the ratio of the feed depth to the metering depth.
5 more elements
Dependencies are inferred from the claim text.